| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | 120°C/h; ISO 75/1 |
|
Polykemi AB SCANAMID 66 A12^ Nylon 66
Information provided by Polykemi AB
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | 120°C/h; ISO 75/1 |
|
Polykemi AB SCANMID 6 B43^ D F15 Nylon 6, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | ISO 75, ASTM D648 |
|
Nilit Nilamid A3 H ZC High Impact PA66
Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | ISO 75-1/-2 |
|
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | |
|
LATI Laticonther 62 GR/50 PA 6, 50% Graphite Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | |
|
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced
Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
205
°C <br>@Thickness 3.20 mm
|
401
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics Ultem 1010A PEI (Asia Pacific)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
205
°C <br>@Thickness 3.20 mm
|
401
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics Ultem 1010A PEI (Europe-Africa-Middle East)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
205
°C <br>@Thickness 3.20 mm
|
401
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
205
°C <br>@Thickness 3.20 mm
|
401
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
205
°C <br>@Thickness 3.20 mm
|
401
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP Stat-kon EE008E PEI
LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
205
°C <br>@Thickness 6.40 mm
|
401
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled
Information provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
205
°C <br>@Thickness 6.40 mm
|
401
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled
PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
205
°C <br>@Thickness 6.40 mm
|
401
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled
Information provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | ASTM D648 |
|
Samyang Tribit® 1551GN15 PBT, Reinforced Flame Retardancy
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN15 is a reinforced, flame retardant g..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66
NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | ISO 75 |
|
Polyram RamLloy PFS301G6 ASA/PBT Alloy, 30% Glass Fiber
30% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | Absolute Drying; ASTM-D648 |
|
Toyobo GLAMIDE® T-422VOR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | dry; ISO 75-1/-2 |
|
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30)
25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | ISO 75-1/-2 |
|
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | ISO 75-1/-2 |
|
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | DAM; ISO 75-1/-2 |
|
DuPont Performance Polymers Zytel® FG50 NC010 Nylon 66
(Unverified Data**)
Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
|
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded
Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | ISO 75 |
|
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | DAM; ISO 75-1/-2 |
|
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**)
36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | ISO 75 |
|
BASF Ultradur S 4090 G4 LS High Speed BK15077 20% Glass Filled PBT |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | 0.25 inch; ASTM D648 |
|
PlastxWorld CEVIAN® A5622 10% GF PA/ABS Alloy, DAM
Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | 0.25 inch; ASTM D648 |
|
PlastxWorld CEVIAN® B2506 30% GF PBT/ABS Alloy
Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc.
|
|||