| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) |
98.9
°C @Thickness 6.35 mm |
210
°F @Thickness 0.250 in |
Unannealed; ASTM D648 |
|
PolyOne Stat-Tech™ AS-08CF/000 Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
|
Network Polymers NPP 30-3500 NA
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
|
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
|
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
|
SABIC Innovative Plastics GELOY HRA222 ASA+PC (Europe-Africa-Middle East)
GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | ASTM D648 |
|
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | ASTM D648 |
|
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hylac® HF143 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
|
Petromont 1100 High Density Polyethylene Resin
Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
|
BP Amoco Acctuf® 3243 Impact Copolymer Polypropylene
(discontinued **)
Suggested fabrication methods: Injection moldingFeatures: General purposeComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
99.0
°C @Thickness 6.40 mm |
210
°F @Thickness 0.252 in |
ASTM D648 |
|
Kingfa HR-527 Modified ABS
Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ISO 75B |
|
Lucite International Diakon® Frost 952 70 Acrylic Polymer
Information provided by Lucite International
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648-95 |
|
Multibase Multi-ABS 3832 Natural
Multi-ABS 3832 is specially formulated for ease of processability, controllability, and thin-walled parts where higher than normal temperatures are being used. This product also shows higher than n..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | Unannealed; ISO 75B-1, -2 |
|
LyondellBasell Hifaxâ„¢ DR279 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ DR279 high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a unique balance of stiffness, impact resistance, processability..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® HDPE TM30 30% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 30% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
99.0
°C @Thickness 3.20 mm |
210
°F @Thickness 0.126 in |
unannealed; ASTM D648 |
|
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
99.0
°C @Thickness 3.20 mm |
210
°F @Thickness 0.126 in |
unannealed; ASTM D648 |
|
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
99.0
°C @Thickness 6.40 mm |
210
°F @Thickness 0.252 in |
ASTM D648 |
|
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
99.0
°C @Thickness 6.40 mm |
210
°F @Thickness 0.252 in |
ASTM D648 |
|
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
99.0
°C @Thickness 6.40 mm |
210
°F @Thickness 0.252 in |
ASTM D648 |
|
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | ASTM D648 |
|
Plastics Group Polifil® C-20 20% Calcium Carbonate-Reinforced Polypropylene
Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resist..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
|
Eastman Tritan MX710 Copolyester
Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | ASTM D648 |
|
CPC - Vycom PROTEC® Homopolymer Polypropylene
Protec HP is a high corrosion resistant polypropylene material which exhibits excellent tensile strength and stiffness at elevated temperatures. Homopolymer polypropylene possesses excellent resista..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | ASTM D648 |
|
Aclo Accutech ABS ABS831G30L Glass Reinforced |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
|
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | ASTM D648 |
|
Aaron Industries AAROPRENE® CFPP 2020 Calcium Carbonate Filled Polypropylene
AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ISO 75-1/-2 |
|
Styrolution Luran® 348 Q Crystal Clear Transparent 77850 SAN
Description: Highly transparent grade with low natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ISO 75-1/-2 |
|
Styrolution Luran® 348 Q Transparent SAN
Description: Highly transparent grade with light natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||