Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 216 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Polymer Resources TP-HG40 Polybutylene Terephthalate, 40% Glass Reinforced Alloy
Polybutylene Terephthalate, 40% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio..
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP COLORCOMP J1000 PES (Europe-Africa-Middle East)
LNP* COLORCOMP* J1000 is a compound based on Polyethersulfone resin.
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Custom Resins Vexel™ 5100 RD PBT; 15% Glass Filled  (discontinued **)
Improved Surface. Property data for dry as molded samples.Data provided by the manufacturer
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Annealed, 0.125 in bars; ASTM D648
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated  (discontinued
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6 CF40 40% Carbon Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAppearance: Black and Natural ColorInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p..
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6 GF33 L N BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: Fast Molding Cycle and LubricatedAppearance: BlackTPCI# 87..
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6 GF35 LE 35% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant Features: Lubricated and Low ExtractablesInformation provided by TP ..
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6/6 GF/M19 HS BK 19% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 19% Filler by Weight and Mineral Filler, 19% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Techmer ES HiFill® TPX-PBT-01055 60% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral Filler, 60% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
<br>@Thickness 3.20 mm
421 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP PFW64 PA 6
LNP* THERMOCOMP* PFW64 is a compound based on Nylon 6 resin containing 20% Glass Fiber, 30% Wollastonite.
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Plastics Group Polifil® 89MRGFHS Glass Fiber and Mineral Reinforced Nylon 6 (DAM)
Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in ind..
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Plastics Group Polifil® 930L-33GF Glass Fiber-Reinforced Nylon 6 (DAM)
Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in ind..
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Cheng Yu Plastic N6C1 Nylon 6, 10% Mineral Reinforced
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612 &nbsp;(Unverified Data**)
33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el..
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Clariant PA213N40 Nylon 6, Mineral/Glass Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Adell BW-37 Nylon 6, 35% Glass Reinforced; Superior Finish
Data provided by Adell Plastics, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Asahi Kasei Thermylon® NSG-440A-H 60% Ceramic and Glass Fiber Reinforced
Information provided by Asahi Thermofil
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
BLUESTAR 201-G25202 PBT, 25% Glass Filled
Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS).
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Bf
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded
BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ISO 75-2
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET
Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, ..
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Annealed, 0.125 in bars; ASTM D648
PolyOne Edgetek® PS-20GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled &nbsp;(discontinued **)
Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® PA6/6 FR 344 BK
Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.