Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 310 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade
Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
RheTech Products GC35P200-01UV 35% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, General Purpose Black
Applications: BracketsStructural componentsHeadlamp housingsWindow frameInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
RheTech Products G20P252-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Black
Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 154 - 168 °C
310 - 335 °F
Average value: 163 °C Grade Count:17
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Deflection Temperature at 0.46 MPa (66 psi) 154 - 162 °C
310 - 324 °F
Average value: 159 °C Grade Count:7
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
Unannealed; ASTM D648
Techmer ES Elastoblend® PA6 IM 409 L MB
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
Spartech PP5430 Glass Fiber Reinforced Homopolymer
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
Unannealed; ASTM D648
Techmer ES HiFill® POM 0223 B Acetal
Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
Unannealed; ASTM D648
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/12 05007 Nylon 612
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
Unannealed; ASTM D648
Chase Plastics CP Pryme® PC320R Polycarbonate, Recycled Content
Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics.
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose
Data provided by Clariant Masterbatches
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
Asahi Kasei Thermylene® P1-35FM-1374H 35% Glass/Fiber Reinforced
Information provided by Asahi Thermofil
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
Asahi Kasei Thermylene® P1-35FM-Y942 35% Glass Fiber/Mineral Reinforced
Information provided by Asahi Thermofil
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
Asahi Kasei Thermylene® P-30FG-0812 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
310 °F
ASTM D648
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural
Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved