| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_7210 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_7220 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_7230 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet FullCure720 Transparent Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet VeroClear FullCure810
Information provided by Proto3000 for their protoyping engineering services.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | ISO 75.1 |
|
Solvay Engineered Polymers DEXFLEX® E756 TPO
(discontinued **)
Description: DEXFLEX® E756 thermoplastic olefinic elastomer (TPO) is designed for extruded automotive air-bag covers. This material provides excellent rigidity, durability and low-temperature toug..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 54.0 °C | 113 - 129 °F | ASTM D648 |
|
DSM Somos® 7110 Epoxy Photopolymer, Green Parts
(discontinued **)
DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LyondellBasell Lupolen® 3010 K LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LyondellBasell Lupolen® 3020 D LDPE
Blow molding, injection molding.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LyondellBasell Lupolen® 3020 F LDPE
Blown film, injection moldings, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LyondellBasell Lupolen® 3020 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LyondellBasell Lupolen® 3020 K LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LyondellBasell Lupolen® 3024 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LyondellBasell Lupolen® 3026 F LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LyondellBasell Lupolen® 3220 K LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LyondellBasell Lupolen® 3412 D LDPE
Telephone cable insulationData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | ASTM D648 |
|
LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade
ApplicationsMicrothene MP564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. MP564189 is 16 mesh powder..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA11
Availability: North AmericaForms: PelletsFeatures: Medium ViscosityTPCI# 6486106Information provided by TP Composites, Inc.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA11 GB7 HS L 7% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 7% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by T..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA11 GL8 HS UV
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Graphite Powder Lubricant and UV StabilizerFeatures: Heat Stabilized. Good UV Resistance and LubricatedAppearance: Natural ColorIn..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
|
EMS-Grivory Grivory® XE 3841 nat PA12
Product description: Grilamid XE 3841 is a flexible, heat stabilized and plasticizer-free Polyamide 12, which offers a very good processability for extrusion. Grilamid XE 3841 is qualified in Europe..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
|
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
|
Dow DNDA-8335 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-8335 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
|
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
|
LATI Latistat 48/9900-03 EVA
Dissipative product based on Ethyl-Vinyl-Acetate (EVA). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
|
|||