| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 45.0 °C | 104 - 113 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 45.0 °C | 104 - 113 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_4410 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 45.0 °C | 104 - 113 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_4510 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 45.0 °C | 104 - 113 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 45.0 °C | 104 - 113 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 45.0 °C | 104 - 113 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 45.0 °C | 104 - 113 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 45.0 °C | 104 - 113 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 41.0 - 45.0 °C | 106 - 113 °F | Average value: 42.6 °C Grade Count:5 |
|
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 41.0 - 45.0 °C | 106 - 113 °F | Average value: 42.9 °C Grade Count:17 |
|
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..
|
|||