Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 54.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 - 54.0 °C
113 - 129 °F
ASTM D648
DSM Somos® 7110 Epoxy Photopolymer, Green Parts  (discontinued **)
DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..
Deflection Temperature at 0.46 MPa (66 psi) 51.0 - 54.0 °C
124 - 129 °F
ASTM D648
3D Systems Accura® 40 Plastic for SLA® Systems
40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a..
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 54.0 °C
104 - 129 °F
Average value: 47.0 °C Grade Count:7
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum ..