| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648-56 |
|
Rotuba 860M Ethyl Cellulose
Data provided by the manufacturer.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ISO 75/Method Bf |
|
Premix Thermoplastics PRE-ELEC® PP 1395
PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resist..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 - 90.0 °C | 180 - 194 °F | after thermal post treatment procedure A; ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer
Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | Unannealed; ASTM D648 |
|
Dow INSPIRE™ DT701-14 TPO
(discontinued **)
High Flow, High Impact TPOInformation provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product l..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 - 195 °C | 180 - 383 °F | Average value: 107 °C Grade Count:46 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
Flint Hills 11R12A Specialty Homopolymer Polypropylene
Features: Good drop impact, radiation resistant. Product does not contain animal derived components and is phthalate-free.Applications: Injection MoldingInformation provided by Flint Hills Resour..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
Flint Hills AP6412-HS Impact Copolymer Polypropylene
High impact copolymer, and FDA compliant. Features: Blush resistant and heat stabilized.Applications: Injection molding: consumer durables, automotive interior trim, furniture trim and housing, and ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
LyondellBasell Petrothene® LM600700 High Density Polyethylene (Blow Molding Grade)
ApplicationsPETROTHENE LM 6007-00 resin exhibits very low taste and odor characteristics as well as good rigidity. Typical applications include water, and milk and juice bottles.Regulatory StatusLM..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
Flint Hills P5M4K-046 Random Copolymer Polypropylene
Random copolymer, FDA compliant.Features: Clarified (50 mil plaque haze 10%), antistat, and controlled rheology.Applications: Injection molding: high clarity parts, medical parts, and good organolep..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
82.0
°C @Thickness 6.40 mm |
180
°F @Thickness 0.252 in |
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics Noryl PX5622 PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
82.0
°C @Thickness 3.20 mm |
180
°F @Thickness 0.126 in |
unannealed; ASTM D648 |
|
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin
Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ISO 75-1/-2 |
|
Styrolution Polystyrol 143 E GR 21 PS
Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman PP 1407L-01 Polypropylene High-Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1407L-01 is a super high-impact copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | Annealed; ASTM D648 |
|
Lubrizol Isoplast® 2510 Engineering Thermoplastic Polyurethane Resin
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product
DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene
DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman PP 1407L-01 Polypropylene High-Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1407L-01 is a super high-impact copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman PP 1407L-01 Polypropylene High-Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1407L-01 is a super high-impact copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene
DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | Annealed; ASTM D648 |
|
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ISO 75-2 |
|
Borealis Daplen™ EE065AI Polypropylene Elastomer Modified
Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natu..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product
DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ISO 75-2 |
|
Borealis RD360MO Polypropylene Random Copolymer, Transparent
RD360MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleating and ant..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
82.0
°C @Thickness 3.17 mm |
180
°F @Thickness 0.125 in |
ISO 75 |
|
A. Schulman FORMION™ FI 397 Ionomer
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene
DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
82.0
°C @Thickness 6.35 mm |
180
°F @Thickness 0.250 in |
ASTM D648 |
|
IRPC Polimaxx Porene AN520 Acrylonitrile Butadiene Styrene
Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets
|
|||