| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746 |
|
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746 |
|
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746 |
|
PolyOne Geon™ HTX M6215 Polyvinyl Chloride Alloy (PVC Alloy)
It is recommended that the compound pellets be dried for 3 to 4 hours at 150 deg. F.Information provided by PolyOne
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746 |
|
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | Average value: 50.0 °C Grade Count:4 |
|
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics GELOY CR7020 ASA (Europe-Africa-Middle East)
GELOY CR7020 is a profile extrusion and co-extrusion grade, blend of ASA/SAN. In co-extrusion it can be used over CYCOLAC, PVC or other compatible polymers.
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East)
Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and ..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
|
|||
| UL RTI, Electrical | 50.0 - 60.0 °C | 122 - 140 °F | Average value: 52.7 °C Grade Count:7 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL746B |
|
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled
Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications.
|
|||
| UL RTI, Electrical |
50.0
°C @Thickness 0.950 - 2.90 mm |
122
°F @Thickness 0.0374 - 0.114 in |
|
|
LG Chemical LUCEL FW700S Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical
|
|||
| UL RTI, Electrical |
50.0
°C @Thickness >=0.750 mm |
122
°F @Thickness >=0.0295 in |
|
|
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity
Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | |
|
LG Chemical LUMIPLAS LD590 Light diffusion ABS
Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific)
Superior Productivity plus heat and impact resistance. Excellent processability.
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific)
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS
LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi.
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East)
DATA ON BK1005 ONLY.
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA
Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance.
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics NORYL PX1390 PPE+PS (Asia Pacific)
Automotive applications, primarily. Excellent electrical properties, easy processability, high heat, 295F (146C) DTUL.
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East)
NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306.
|
|||
| UL RTI, Electrical |
50.0
°C @Thickness 1.50 mm |
122
°F @Thickness 0.0591 in |
UL 746 |
|
Teknor Apex APEX® 7500-85 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL Q..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746 |
|
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| UL RTI, Electrical | 50.0 - 130 °C | 122 - 266 °F | Average value: 119 °C Grade Count:3 |
|
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific)
ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL.
|
|||
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
|
SABIC Innovative Plastics NORYL FN150 PPE+HIPS (Europe-Africa-Middle East)