| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Electrical |
105
°C @Temperature 105 °C |
221
°F @Temperature 221 °F |
UL 746 |
|
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid)
Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: ..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS
PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components.
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC810SK is suitable for those applications that require sparkl..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® FXC810SL PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810SL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require sparkle colour effects with lowered RFI inhibitor. Colour package may effect perform..
|
|||
| UL RTI, Electrical |
105
-
105
°C @Temperature 105 - 105 °C |
221
-
221
°F @Temperature 221 - 221 °F |
Average value: 105 °C Grade Count:1 |
|
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific)
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics ULTEM 2212EPR PEI
20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising.
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Ultem 2313 PEI
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region...
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics ULTEM CRS5201 PEI (Europe-Africa-Middle East)
20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics NORYL N300X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Noryl 731H PPE+PS
High gloss, general purpose grade. 130C (266F) DTUL. UL 94 HB rated. For multiple plugs, wine filter plates, etc.This data was supplied by SABIC-IP for the Americas region.
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics NORYL 731S PPE+PS (Asia Pacific)
High heat PPO/HIPS alloy suitable for use in some potable water applications.
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
|
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene
DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
|
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass)
DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch..
|
|||
| UL RTI, Electrical |
105
°C @Thickness 0.780 mm |
221
°F @Thickness 0.0307 in |
UL 94 |
|
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene
DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman.
|
|||
| UL RTI, Electrical |
105
°C @Thickness 0.780 mm |
221
°F @Thickness 0.0307 in |
UL 94 |
|
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene
DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman.
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
|
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene
DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
|
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene
DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman.
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
|
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene
DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b..
|
|||
| UL RTI, Electrical |
105
°C @Thickness 0.780 mm |
221
°F @Thickness 0.0307 in |
UL 94 |
|
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene
DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman.
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
|
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene
DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b..
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized
|
|||
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
|
SABIC Innovative Plastics NORYL ENG265 PPE+PS
PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a..
|
|||