Polymer Property : UL RTI, Electrical = 221 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
UL RTI, Electrical 105 - 105 °C

@Temperature 105 - 105 °C
221 - 221 °F

@Temperature 221 - 221 °F
Average value: 105 °C Grade Count:1
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..