| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® EX39F ABS
Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East)
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® FR15 ABS
Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® FR23 ABS
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® G151 ABS (Europe-Africa-Middle East)
CYCOLAC G151 is a flame retardant grade of ´new technology´ CYCOLAC which has been especially formulated to minimise many of the problems often associated with the processing of traditiona..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East)
CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® MG47N ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® MG94 ABS
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® S701S ABS (Europe-Africa-Middle East)
CYCOLAC S701S is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appl..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East)
CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East)
CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according ..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East)
UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Europe-Africa-Middle East)
Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties for a wide variety of applications including business equipment, TVs, monitors, enclosures, among others..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific)
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CY4000 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CY4000 resin is an injection moldable, flame retardant PC/ABS blend free of brominated or chlorinated flame resistant additives. Cycoloy CY4000 has excellent flow and balanced impact proper..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East)
CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® EX58 ABS
High impact ABS for sheet extrusion and blow molding applications.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific)
High impact and ductility at 73F (23C) and -20F (-29C).
|
|||
| UL RTI, Mechanical with Impact |
60.0
°C @Thickness 1.60 mm |
140
°F @Thickness 0.0630 in |
UL746B |
|
Ineos ABS Lustran® 266 Specialty, Transparent
(discontinued **)
A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and va..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
LG Chemical HI121H ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
60.0
°C @Thickness >=1.50 mm |
140
°F @Thickness >=0.0591 in |
|
|
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
|
|||
| UL RTI, Mechanical with Impact |
60.0
°C @Thickness >=0.750 mm |
140
°F @Thickness >=0.0295 in |
|
|
LG Chemical LUPOY HP5004A PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | |
|
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned
Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | |
|
Covestro Bayblend® T 65 Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C1100 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1100 is a PC+ABS blend developed to satisfy the demanding application requirements, where optimum combination is needed of superior processing efficiency, excellent ductility also at sub ze..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
|
|||