| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® 153 PC
Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized.
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® BY2710X PC (Asia Pacific)
BY2710X is a modified Polycarbonate (PC) resin. It is a non-filled, injection moldable grade with UL-94 V0 rating and is available in various opaque color options.
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® EXL9330P PC COPOLYMER (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | |
|
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | |
|
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® HF1110R PC (Europe-Africa-Middle East)
LEXAN HF1110R is a high flow grade especially designed for applications that require thin wall sections and high flow lengths.
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® 151 PC (Asia Pacific)
Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® 923X PC
Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur..
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | |
|
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | |
|
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | |
|
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, ..
|
|||
| UL RTI, Mechanical with Impact | 115 - 150 °C | 239 - 302 °F | Average value: 131 °C Grade Count:9 |
|
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | Minimum thickness 0.040 inches. |
|
LyondellBasell Pro-fax 6524 Polypropylene Homopolymer, Heat- and Extraction-Resistant
Key Features: heat and extraction-resistant polypropylene homopolymer resin, FDA acceptable, high resistance to solventsApplications: appliances, automotive under-the-hood applicationsMeets FDA requ..
|
|||
| UL RTI, Mechanical with Impact |
115
°C @Thickness 3.00 mm |
239
°F @Thickness 0.118 in |
ASTM UL94 |
|
LyondellBasell Astryn BA45H Polypropylene Copolymer, Flame Retardant
Key Features: medium melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colorability..
|
|||
| UL RTI, Mechanical with Impact |
115
°C @Thickness 1.60 mm |
239
°F @Thickness 0.0630 in |
|
|
LyondellBasell Higlass SB224-1 Polypropylene Copolymer, 10% Glass Fiber
Key Features: conventional melt flow, medium modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, excellent impact strength, good processabilityApplications: automotive wheel..
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
SABIC Innovative Plastics Ultem ATX100R PEI+PCE
Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Americas region.
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE (Asia Pacific)
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant.
|
|||
| UL RTI, Mechanical with Impact |
115
°C @Thickness 1.47 mm |
239
°F @Thickness 0.0579 in |
UL 746B |
|
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin
Thin-wall injection moldings grade of high fluidity. It has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Comparatively large-size components of mechanic..
|
|||
| UL RTI, Mechanical with Impact |
115
°C @Thickness 1.47 mm |
239
°F @Thickness 0.0579 in |
UL 746B |
|
Teijin Panlite® LN-1250G Flame Resistant, Translucent Polycarbonate Resin
Flame retardant and mold release grade with normal fluidity, which is suitable for injection molding applications.Applications:Electric, electronic and business machine components that need flame re..
|
|||
| UL RTI, Mechanical with Impact |
115
°C @Thickness 1.47 mm |
239
°F @Thickness 0.0579 in |
UL 746B |
|
Teijin Panlite® LV-2225Y Standard (mold release/ice color grade) Polycarbonate Resin
Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity.Appl..
|
|||
| UL RTI, Mechanical with Impact |
115
°C @Thickness 1.47 mm |
239
°F @Thickness 0.0579 in |
UL 746B |
|
Teijin Panlite® L-1250ZW Extrusion Grade Polycarbonate Resin
Information provided by Teijin Chemicals Ltd.
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | |
|
Covestro Makrolon® 2607 Polycarbonate, Injection Grade
Easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially a..
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
Covestro Makrolon® 2665 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy..
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
Covestro Makrolon® 2805 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
|
|||
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
|
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
|
|||
| UL RTI, Mechanical with Impact |
115
°C @Thickness 1.50 mm |
239
°F @Thickness 0.0591 in |
|
|
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se..
|
|||
| UL RTI, Mechanical with Impact |
115
°C @Thickness 2.50 mm |
239
°F @Thickness 0.0984 in |
746B |
|
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned)
Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl..
|
|||
| UL RTI, Mechanical with Impact |
115
°C @Thickness 1.50 mm |
239
°F @Thickness 0.0591 in |
746B |
|
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry)
Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl..
|
|||