| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | Average value: 65.0 °C Grade Count:3 |
|
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
|
|||
| UL RTI, Mechanical with Impact | 65.0 - 80.0 °C | 149 - 176 °F | Average value: 72.5 °C Grade Count:3 |
|
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | Minimum thickness of 0.059 inches. |
|
LyondellBasell Pro-fax SD242 Polypropylene Impact Copolymer
Key Features: short cycle times for high productivity, good cold impact resistance, good stiffness and impact balance, high flow ease of mold filling and minimum warpage, low odor and low taste tran..
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | Minimum thickness of 0.059 inches. |
|
LyondellBasell Pro-fax SG702 Polypropylene Impact Copolymer
Key Features: excellent cold impact resistance, good stiffness and impact balance, UV stabilizer, polypropylene copolymer resin, injection moldingApplications: automotive interior trim, pet carriers..
|
|||
| UL RTI, Mechanical with Impact |
65.0
°C @Thickness 0.750 - 0.820 mm |
149
°F @Thickness 0.0295 - 0.0323 in |
|
|
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant
Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
65.0
°C @Thickness 0.750 - 0.820 mm |
149
°F @Thickness 0.0295 - 0.0323 in |
|
|
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant
Feature: Injection Molding, PA66+GF10%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
|
|||
| UL RTI, Mechanical with Impact |
65.0
°C @Thickness >=0.750 mm |
149
°F @Thickness >=0.0295 in |
|
|
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose
Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
65.0
°C @Thickness >=0.750 mm |
149
°F @Thickness >=0.0295 in |
|
|
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose
Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
65.0
°C @Thickness >=0.750 mm |
149
°F @Thickness >=0.0295 in |
|
|
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose
Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
65.0
°C @Thickness >=1.50 mm |
149
°F @Thickness >=0.0591 in |
|
|
LG Chemical LUPOL GP2200 PP+GF20%
Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
|
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
|
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, Dry as Molded
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
|
SABIC Innovative Plastics NORYL RN0401 PPE+PS
Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only.
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
|
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East)
LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized.
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
|
SABIC Innovative Plastics LNP THERMOCOMP UF007AS PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF007AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include Heat Stabilized .
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
|
SABIC Innovative Plastics NORYL ENV150 PPE (Europe-Africa-Middle East)
Noryl* ENV150 modified polyphenylene ether resin is an unfilled, flame retardant high heat grade suitable for extrusion molding conversion route. It uses non-chlorinated, non-brominated FR additives..
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
|
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific)
Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl ..
|
|||
| UL RTI, Mechanical with Impact |
65.0
°C @Thickness 0.780 mm |
149
°F @Thickness 0.0307 in |
UL 746 |
|
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman.
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
|
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded
Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
|
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar.
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
|
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
|
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
|
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded
Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar.
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
|
Arkema Group Rilsan® BECN TL Nylon 11, Sheathing Grade (Conditioned)
Designation ISO 1874-PA11,KHL,12-010Rigid grade for sheathing of wires and cables. Available color: natural. Light and heat stabilized.High abrasion resistance. Well adapted melt viscosity. Ability ..
|
|||
| UL RTI, Mechanical with Impact |
65.0
°C @Thickness 1.50 mm |
149
°F @Thickness 0.0591 in |
746B |
|
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry)
Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
|
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
|
|||
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
|
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
|
|||
| UL RTI, Mechanical with Impact |
65.0
°C @Thickness >=0.750 mm |
149
°F @Thickness >=0.0295 in |
|
|
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose
Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical
|
|||