| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS
PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific)
PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® BFL2000 PC
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East)
Transparent/translucent PC for light diffusion special effects. Color package may affect performance.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® FXE4271L PC (Asia Pacific)
Lexan* FXE4271L is a 10% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac..
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® FXM121R PC
PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® HF1130R PC (Europe-Africa-Middle East)
LEXAN HF1130R is a high flow, UV stabilized, grade especially designed for applications that require thin wall sections and higher flow lengths.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific)
18 MFR. Improved flame retardance. Internal mold release. UV stabilized.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific)
7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® BFL2000U PC (Asia Pacific)
Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig..
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® FL2003 PC (Asia Pacific)
Various weight reductions at 0.250" (6.35mm) wall. Low temperature impact and high heat resistant. Excellent surface. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region...
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C @Thickness 0.500 - 2.50 mm |
176
°F @Thickness 0.0197 - 0.0984 in |
|
|
LG Chemical Lupoy 3030-10 Polycarbonate Resin
Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | |
|
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by ..
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | |
|
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p..
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | |
|
LG Chemical LUPOY GP2300 PC+GF30%, Heat Resistance
Description: Injection Molding, PC+GF30%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics NORYL SE100 PPE+HIPS (Europe-Africa-Middle East)
NORYL® SE100 is an unfilled, flame retardant material with a Vicat B/120 of 120°C. It has a UL-94 flammability rating V1 @ 1.47 mm, and is halogen free according to VDE/DIN 472 part 815.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics NORYL SE100X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/V1 rated. RTI Elec/Imp/Str 95/80/95. Good flow. Suitable for E/E market indoor/outdoor applications.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC
LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled material.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics LNP LUBRILOY Lexan_WR6300 AES+PC+SAN
LNP* Lubriloy* Lexan_WR6300 compound is a wear resistant PC+SAN, with proprietary lubricant, for business equipment applications.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics LNP STAT-KON DX89795 PC (Europe-Africa-Middle East)
LNP* STATKON* DX89795 is a compound based on Polycarbone resin containing Carbon Powder. Added features include: Electrically Conductive, Easy Molding, Mold Release.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics NORYL N225X PPE+PS
PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications.
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics NORYL PX1007 PPE+PS
Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade.
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C @Thickness 1.50 mm |
176
°F @Thickness 0.0591 in |
UL 746B |
|
Diamond Polymers ABS 3502
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C @Thickness 1.50 mm |
176
°F @Thickness 0.0591 in |
UL 746B |
|
Diamond Polymers ABS 7502
Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C @Thickness 1.47 mm |
176
°F @Thickness 0.0579 in |
UL 746B |
|
Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin
CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica..
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
|
|||
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
|
SABIC Innovative Plastics NORYL PX1005X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications.
|
|||