| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746 |
|
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746 |
|
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746 |
|
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® FR15U ABS
Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60).
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS (Asia Pacific)
PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1...
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics GELOY HRA222F ASA+PC
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific)
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746 |
|
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| UL RTI, Mechanical without Impact |
90.0
°C @Thickness 0.750 mm |
194
°F @Thickness 0.0295 in |
UL-746B |
|
Shell Carilon® D26FX100 Polyketone, General-Purpose Extrusion Grade
(discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26FX100 is a general-purpose extrusion grade with mechanical properties that classify it as an eng..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Asia Pacific)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
|
|||
| UL RTI, Mechanical without Impact |
90.0
°C @Thickness 1.50 mm |
194
°F @Thickness 0.0591 in |
UL 746B |
|
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin
Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | |
|
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR
Information provided by Samsung Cheil Industries.
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | |
|
Samsung Cheil Industries Infino® NH-1015 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | |
|
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR
Information provided by Samsung Cheil Industries.
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746 |
|
Teknor Apex APEX® 4109 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics NORYL GFN2 PPE+PS
PPE+PS blend. 20% Glass reinforced. UL746C F1. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional sta..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics NORYL GFN1 PPE+PS
PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui..
|
|||
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
|
SABIC Innovative Plastics NORYL GFN3 PPE+PS
PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui..
|
|||
| UL RTI, Mechanical without Impact |
90.0
°C @Thickness 3.20 mm |
194
°F @Thickness 0.126 in |
UL746B |
|
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o..
|
|||
| UL RTI, Mechanical without Impact |
90.0
°C @Thickness 1.50 mm |
194
°F @Thickness 0.0591 in |
UL-746B |
|
Axiall HF-6597 Rigid PVC, Molding
Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information provide..
|
|||
| UL RTI, Mechanical without Impact |
90.0
°C @Thickness 1.40 mm |
194
°F @Thickness 0.0551 in |
UL-746B |
|
Axiall MP-6510 Rigid PVC, Molding
Georgia Gulf MP-6510 is a maximum properties electrical grade PVC injection molding compound processing excellent strength and toughness. In addition, it has good processing stability and surface a..
|
|||
| UL RTI, Mechanical without Impact |
90.0
°C @Thickness 1.40 mm |
194
°F @Thickness 0.0551 in |
UL-746B |
|
Axiall SP-7107 Rigid PVC, Molding
Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it ..
|
|||
| UL RTI, Mechanical without Impact |
90.0
°C @Thickness 0.750 mm |
194
°F @Thickness 0.0295 in |
UL-746B |
|
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it ..
|
|||