| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Pour Point | <= -34.4 °C | <= -30.0 °F | D97 |
|
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid
Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he..
|
|||
| Pour Point | <= -34.4 °C | <= -30.0 °F | D97 |
|
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid
Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
Lubriplate AC-0 Petroleum-Based Air Compressor Fluid
Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
Lubriplate FMO 150 AW USP Mineral Oil-Based Food Machinery Grade Oil
For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
Lubriplate H0-0 Petroleum-Based Heavy-Duty Hydraulic Oil
Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
Lubriplate SPO-222 Petroleum-Based Gear, Bearing, & Recirculating Oil
Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubricati..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
Lubriplate STO 4 Oil Food Machinery Oil
Special, non-corrosive oil for lubricating stirrups on bottle filling machines. Class H-2.**Available in Bottles, Jugs, Pails, 1/4 Drums and DrumsH-1 Class Lubricants are manufactured with ingredien..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
Lubriplate NO.2 Petroleum-Based Machine Tool Oil
Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips SynXPA® 150 R&O Oil
Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acti..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips 46 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear Diamond Class® 68 AW Turbine Oil
Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 1 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 1
Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 100 Gas Compressor Fluid
Description: Conoco Hydroclear Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality hydrocracked base oil, combi..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 100 Multipurpose R&O Oil, AGMA Lubricant No. 3
Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear ..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 2 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 2
Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 46 Multipurpose R&O Oil, AGMA Lubricant No. 1
Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidation inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 68 2 EP gear Oil
Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 68 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 68 Multipurpose R&O Oil, AGMA Lubricant No. 2
Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear ..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 68 Turbine Oil
Description: Conoco Hydroclear Turbine Oil is a premium rust- and oxidationinhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Turbine Oil is specially formula..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® El Mar® 15W-40 Ashless Supreme
Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is speci..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® El Mar® 15W-40 Low Ash Heavy Duty
Description: Conoco Hydroclear El Mar Low Ash Heavy Duty is a high-quality low ash natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Low Ash Heavy Du..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® El Mar® 40 Ashless Supreme
Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is speci..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® El Mar® Low Ash Heavy Duty SAE 40
Description: Conoco Hydroclear El Mar Low Ash Heavy Duty is a high-quality low ash natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Low Ash Heavy Du..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips 46 Ultra-Clean Super Hydraulic Oil
Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear Diamond Class® 68 Turbine Oil
Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 100 3 EP gear Oil
Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 3 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 3
Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 32 Rock Oil
Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill ..
|
|||
| Pour Point | -34.4 °C | -30.0 °F | |
|
ConocoPhillips Hydroclear® 46 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
|
|||