| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Pour Point | -42.0 °C | -43.6 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 275L (SO) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -42.0 °C | -43.6 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 761G Grease
Information provided by Nye Lubricants.
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil 11M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil 15M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil 627 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil Gargoyle Arctic 155
Gargoyle Arctic 155, C Heavy and 300 products are high performance naphthenic mineral oils primarily intended for use in refrigeration compressors. They have low pour points and excellent fluidity a..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil Gargoyle Arctic 300
Gargoyle Arctic 155, C Heavy and 300 products are high performance naphthenic mineral oils primarily intended for use in refrigeration compressors. They have low pour points and excellent fluidity a..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | |
|
ExxonMobil Mobil Clean 5W-20 7500
Mobil Clean 7500 is formulated from a combination of synthetic and conventional quality base stocks combined with modern performance additives, including an advanced cleaning additive system to prov..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | |
|
ExxonMobil Mobil Clean 5W-30 7500
Mobil Clean 7500 is formulated from a combination of synthetic and conventional quality base stocks combined with modern performance additives, including an advanced cleaning additive system to prov..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil 46 Mobil EAL Arctic Series
Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ChevronTexaco 1000 THF Tractor Hydraulic Fluid
FeaturesChevron 1000 THF (formerly Chevron Tractor Hydraulic Fluid and Amoco 1000 Fluid) is a high quality, multifunctional fluid, specially formulated for use in transmissions, final drives, wet br..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ChevronTexaco HiPerSYN™ ISO 46 Oil
FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ChevronTexaco HiPerSYN™ ISO 68 Oil
FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ChevronTexaco Mechanism LPS® ISO 46 Hydraulic Oil
Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ChevronTexaco Mechanism LPS® ISO 68 Hydraulic Oil
Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | |
|
ChevronTexaco URSA® SAE 10W Super Plus
Texaco Ursa Super Plus oils deliver value through:Oil lasts longer between drains — Good oxidation stability protects against oil thickening during manufacturers recommended oil drain periods.Vital..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ChevronTexaco Vistac® ISO 32 Rock Drill Oil
FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil 46 Mobil EAL Arctic Series
Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil 634 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil Gargoyle Arctic 155
Gargoyle Arctic 155, C Heavy and 300 products are high performance naphthenic mineral oils primarily intended for use in refrigeration compressors. They have low pour points and excellent fluidity a..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | |
|
ExxonMobil Mobil Clean 5W-30 7500
Mobil Clean 7500 is formulated from a combination of synthetic and conventional quality base stocks combined with modern performance additives, including an advanced cleaning additive system to prov..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil Mobilfluid 424
Mobilfluid 424 is an extra high performance multipurpose tractor lubricant engineered to meet or exceed transmission and hydraulic fluid requirements. The advanced technology in Mobilfluid 424 is ..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ChevronTexaco SAE 75W-90 Manual Transaxle Fluid GL-4
FeaturesChevron Manual Transaxle Fluid GL-4 is a multipurpose lubricant.Chevron Manual Transaxle Fluid GL-4 is formulated with ISOSYN® base stocks and synthetic polymer to meet the severe demands o..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil 630 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil 636 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil Gargoyle Arctic 300
Gargoyle Arctic 155, C Heavy and 300 products are high performance naphthenic mineral oils primarily intended for use in refrigeration compressors. They have low pour points and excellent fluidity a..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | |
|
ChevronTexaco URSA® SAE 10W-30 Super Plus
Texaco Ursa Super Plus SAE 10W-30 delivers value through:One oil for all services, both diesel and gasoline, minimizes the chance of misapplication.Reduced inventory investment — No need to maintai..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ExxonMobil 526 Mobil SHC 500 Series
Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. ..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | ASTM D97 |
|
ChevronTexaco Rykon® ISO 68 Premium Oil
FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion ..
|
|||
| Pour Point | -42.0 °C | -43.6 °F | |
|
ChevronTexaco URSA® SAE 10W Extra Duty
Texaco Ursa Extra Duty oils deliver value through:Excellent high temperature deposit control. Protects against high temperature oxidation and oil thickening.Special extreme pressure antiwear propert..
|
|||