| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 188B (SO) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 274VL (SO) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 368A (NC-GP) (RL) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 368AX-1 (RL) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 368AX-F (RL) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 368SM (RL) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 609 (SO) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 774F-1 (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 774VLF (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 774VLF-MS (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 774VLF-UV(NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 774VLF-WHITE (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 774VL-MS (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 868VL (FG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | -43.0 °C | -45.4 °F | Base Oil; ASTM D97 |
|
Nye Lubricants 774VL (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Pour Point | <= -43.0 °C | <= -45.4 °F | ASTM D97 |
|
ExxonMobil Mobil Rarus 826
The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet..
|
|||
| Pour Point | -43.0 °C | -45.4 °F | |
|
Dow Corning XIAMETER® PMCPPMX-200 30,000CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 30,000CS. 100% active, 30,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
|
|||
| Pour Point | -43.0 °C | -45.4 °F | ASTM D97 |
|
ChevronTexaco Delo® 400 Synthetic, SAE 5W-40
Chevron Delo 400 Synthetic heavy duty motor oils are multipurpose 100% synthetic lubricants formulated for use in gasoline and diesel engines, torque converters, gear cases, and hydraulic systems op..
|
|||
| Pour Point | <= -43.0 °C | <= -45.4 °F | ASTM D97 |
|
ExxonMobil Mobil Rarus 826
The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet..
|
|||