| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glow Wire Test | 675 - 960 °C | 1250 - 1760 °F | Average value: 820 °C Grade Count:6 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
|
|||
| Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 783 °C Grade Count:6 |
|
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
|
|||
| Glow Wire Test | 725 - 960 °C | 1340 - 1760 °F | Average value: 816 °C Grade Count:4 |
|
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
|
|||
| Glow Wire Test | 775 - 960 °C | 1430 - 1760 °F | Average value: 868 °C Grade Count:8 |
|
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
|
|||
| Glow Wire Test | 850 - 960 °C | 1560 - 1760 °F | Average value: 919 °C Grade Count:8 |
|
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
|
|||
| Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 746 °C Grade Count:52 |
|
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
|
|||
| Glow Wire Test | 390 - 960 °C | 734 - 1760 °F | Average value: 685 °C Grade Count:19 |
|
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 871 °C Grade Count:8 |
|
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
|
|||
| Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 865 °C Grade Count:7 |
|
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
|
|||
| Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 871 °C Grade Count:3 |
|
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
|
|||
| Glow Wire Test | 649 - 960 °C | 1200 - 1760 °F | Average value: 762 °C Grade Count:10 |
|
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
|
|||
| Glow Wire Test | 825 - 960 °C | 1520 - 1760 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics LNP LUBRICOMP OFL38A PPS - Branched (Europe-Africa-Middle East)
LNP* LUBRICOMP* OFL38A is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features include : Internally Lubricated.
|
|||
| Glow Wire Test | 875 - 960 °C | 1610 - 1760 °F | IEC 60695-2-13 |
|
SABIC Innovative Plastics LNP LUBRICOMP OFL38A PPS - Branched (Europe-Africa-Middle East)
LNP* LUBRICOMP* OFL38A is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features include : Internally Lubricated.
|
|||
| Glow Wire Test | 775 - 960 °C | 1430 - 1760 °F | Average value: 866 °C Grade Count:3 |
|
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 869 °C Grade Count:11 |
|
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
|
|||
| Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 857 °C Grade Count:3 |
|
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
|
|||
| Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 753 °C Grade Count:3 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
|
|||
| Glow Wire Test | 750 - 960 °C | 1380 - 1760 °F | Average value: 915 °C Grade Count:4 |
|
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
|
|||
| Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 903 °C Grade Count:13 |
|
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
|
|||