| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D746 |
|
PolyOne FireCon™ CPE 30-11 REV 2 Polyethylene, Chlorinated (CPE)
CPE-30-11 REV 2 is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-11 REV 2 offers high tensile and superior fluid res..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D746 |
|
PolyOne FireCon™ CPE 30-2 RoHS BLACK Polyethylene, Chlorinated (CPE)
CPE-30-2 RoHS BLACK is a RoHS compliant heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-2 RoHS BLACK has a good balance ..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D746 |
|
PolyOne Geon™ Vinyl Flexible MG23B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D746 |
|
PolyOne Geon™ Vinyl Flexible XV 1144 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TCP Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-95 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D746 |
|
PolyOne Geon™ Vinyl Flexible F80E Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Brittleness Temperature | <= -35.0 °C | <= -31.0 °F | 0% Failure Rate; ASTM D746 |
|
NOVA Chemicals Novapol® LM-4021-L LDPE Injection Molding Resin
Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat..
|
|||
| Brittleness Temperature | <= -35.0 °C | <= -31.0 °F | ASTM D 746 |
|
Karina Karintox 70/2 Polyolefin Compound
Halogen free, fire retardant, low smoke and fume polyolefinic compound. Recommended for insulation of electrical cables up to 1KV.Information provided by Karina Indústria e Comércio de Plá..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D746 |
|
LyondellBasell Microthene® G MN72700 Low Density Polyethylene
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | F<sub>50</sub>, Test method has been found useful for specification purposes, but does not necessarily indicate the lowest temperature at which the material may be used.; ASTM D746 |
|
LyondellBasell Petrothene® NA860241 Low Density Polyethylene
ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | |
|
Sylvin Technologies 6400-85 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
|
|||
| Brittleness Temperature | <= -35.0 °C | <= -31.0 °F | |
|
Sibur Neva Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | DIN 53546 |
|
Lubrizol ESTANE® T4065 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D746 |
|
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer
A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | Cold Flex; ISO 458/2 |
|
Fainplast Compounds GS 64 Flexible PVC, Injection Molding for Footwear
Soles
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | Cold Flex; ISO 458/2 |
|
Fainplast Compounds GS 65/T Flexible PVC, Injection Molding for Footwear
Crystal soles and sandals
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | Cold Flex; ISO 458/2 |
|
Fainplast Compounds GS 69/F Flexible PVC, Injection Molding for Footwear
Sandals
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D746 |
|
Colorite Polymers CS6019GP Non Lead Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D-746 |
|
Axiall 8642 Moldings & Extrusions Flexible PVC
General purpose, fungus resistant extrusion and molding compound recommended for weatherstrips and tubings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D-746 |
|
Axiall 8805 Moldings & Extrusions Flexible PVC
General purpose clear extrusion compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D-746 |
|
Axiall 12812 Moldings & Extrusions Flexible PVC
General purpose, flame retardant extrusion compound formulated for good oil resistance. Also suitable for general purpose 80°C rated jacketing applications.Information provided by Georgia GulfGeor..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D-746 |
|
Axiall 22851 Coax & Telecom Flexible PVC
Non-lead stabilized, flame retardant jacket compound. Best suited for CM, CMR applications over FR PVC. Maximum service temperature rating of 75°C. UL recognized for 720 hr sunlight resistance.I..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D-746 |
|
Axiall 8758 Moldings & Extrusions Flexible PVC
A general purpose extrusion compound recommended for extruded shapes, weatherstrips and flexible gaskets. Formulated for good UV light resistance and low temperature properties.Information provided..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D-746 |
|
Axiall 8780 Moldings & Extrusions Flexible PVC
Low gravity, general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D-746 |
|
Axiall 10701 Wire & Cable Flexible PVC
General purpose 80°C compound with good low temperature properties recommended for 15 mil wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D-746 |
|
Axiall 12791 Wire & Cable Flexible PVC
General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties and 720 hour sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall ..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D-746 |
|
Axiall 18731 Wire & Cable Flexible PVC
Non-lead stabilized, UL recognized 720 hour sunlight resistant in all colors, 105 C rated jacket compound with good low temperature performance.Information provided by Georgia GulfGeorgia Gulf becam..
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | Cold Flex; ISO 458/2 |
|
Fainplast Compounds PH 62 Flexible PVC, Transparent Extrusion
Transparent profiles
|
|||
| Brittleness Temperature | -35.0 °C | -31.0 °F | Cold Flex; ISO 458/2 |
|
Fainplast Compounds PMP 75/OP Flexible PVC, Extrusion Modified with PU
High resistance to oil and hydrocarbon, with good abrasion resistance and elasticity
|
|||