| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
PolyOne Geon™ Vinyl Wire & Cable EC486 DA Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
|
|||
| Brittleness Temperature | -45.0 - -40.0 °C | -49.0 - -40.0 °F | Average value: -43.3 °C Grade Count:3 |
|
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m..
|
|||
| Brittleness Temperature | <= -45.0 °C | <= -49.0 °F | TPE-0089 (ASTM D 746) |
|
Advanced Elastomer Systems Santoprene® 253-50 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
Eastman 18BOA Polyethylene
(discontinued **)
Polyethylene 18BOA is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic mold..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
Eastman 811P Polyethylene
(discontinued **)
Injection grade. With its high melt index, the material flows well in molding machines and fills large molds with ease. It is used for molding housewares and other items where a flexible, easy mol..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
LyondellBasell Microthene® G MN71020 Low Density Polyethylene
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D638 |
|
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder
Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
Teknor Apex Flexalloy® 3500-65 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
Teknor Apex Flexalloy® 89501-83 Polyvinyl Chloride, Elastomer
Notes: 105°C Insulation; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility Uses Wet Rated Insulation Wire Types: NISPE-1; NISPE-2; SE; SEO; SEOW; SEW; SJ..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
Teknor Apex Flexalloy® 9900-55 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics ..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
Colorite Polymers Weatherflex™ CS1534WX (NTL02P) Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | Temperature Retraction, TR-10 |
|
Dow Nordel® IP 4570 General Purpose Compound
FormulationNordel® IP 4570
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
Colorite Polymers MULTICHEM™ 8014 Vinyl-Urethane Blend
Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers.
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
|
Alliance Polymers Zythane™ 5060A Thermoplastic Polyurethane Elastomer
Zythane™ 5060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746; ISO 812 |
|
Advanced Polymer Alloys Alcryn® 3065 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D-746 |
|
Axiall 11600 Wire & Cable Flexible PVC
Clear, non-staining speaker wire insulation and general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | Brittle point |
|
Dow Advanta® 3650 Specialty Elastomer
(discontinued **)
Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000..
|
|||
| Brittleness Temperature | -45.0 °C | -49.0 °F | |
|
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi..
|
|||