Polymer Property : Brittleness Temperature = -62.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Brittleness Temperature <= -62.0 °C
<= -79.6 °F
TPE-0089 (ASTM D 746)
ExxonMobil Santoprene® 8211-35W237 Thermoplastic Rubber &nbsp;(discontinued **)
A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe..
Brittleness Temperature -62.0 °C
-79.6 °F
ASTM D746
Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber &nbsp;(discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
Brittleness Temperature -62.0 °C
-79.6 °F
ISO 974
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET &nbsp;(Unverified Data**)
Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme..
Brittleness Temperature <= -62.0 °C
<= -79.6 °F
ASTM D2236
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride &nbsp;(discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Brittleness Temperature -62.0 °C
-79.6 °F
ASTM D746
PolyOne Synprene® RT-3880M Styrene Butadiene Block Copolymer (SBC) &nbsp;(discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Brittleness Temperature <= -62.0 °C
<= -79.6 °F
ASTM D746
SCG Chemicals EL-Leneâ„¢ H6240B High Density Polyethylene Blow Molding
Key Characteristics:Good stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthGood appearanceOdorlessSafe for food contactGood printabilityRecommended App..
Brittleness Temperature -62.0 °C
-79.6 °F
ASTM D 746
Zylog Neoplast® 145 FT EB Thermoplastic Vulcanizate
Neoplast 145 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, ..
Brittleness Temperature -62.0 °C
-79.6 °F
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Brittleness Temperature -62.0 °C
-79.6 °F
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Brittleness Temperature -62.0 °C
-79.6 °F
ASTM D746
PolyOne Synprene® RT-3975 Thermoplastic Elastomer - SBC &nbsp;(discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti..
Brittleness Temperature -62.0 °C
-79.6 °F
ASTM D746
PolyOne Synprene® RT-3985 Thermoplastic Elastomer - SBC &nbsp;(discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti..