| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene
Clearflex FF D0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FF D0 are highly transparent, have excellent sealing properties,..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene
Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Polimeri Europa Clearflex® FG B3 Very Low Density Polyethylene
Clearflex FG B3 is a linear low density polyethylene, with antioxidants, slip and antiblocking agents, suitable for blown film technology. The product is characterized by a very low density and a h..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Polimeri Europa Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T CLH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CLH 108 show e..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Polimeri Europa Clearflex® MP D0 Very Low Density Polyethylene
Clearflex MP D0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati..
|
|||
| Brittleness Temperature | -70.0 °C | -94.0 °F | ASTM D 746 |
|
Polyplastic Armobond® PE 2K Polyethylene Adhesive Compound
Information provided by PolyPlastic Group.
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | F<sub>0</sub> notched specimen; ASTM D746 |
|
NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin
Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffnessApplications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert a..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
|
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin
Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer.
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D 746 |
|
NOVA Chemicals Sclair® 31G Butene Copolymer LLDPE Extrusion Coating Resin
31G complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 31G is su..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Polimeri Europa Clearflex® CL B0 Very Low Density Polyethylene
Clearflex CL B0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has a high stretchability and a good cling effect.Main Applications: C..
|
|||
| Brittleness Temperature | >= -70.0 °C | >= -94.0 °F | ASTM D746 |
|
ExxonMobil LL 6235 Injection Molding Resin
(discontinued **)
LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in ..
|
|||
| Brittleness Temperature | -70.0 °C | -94.0 °F | ASTM D746 |
|
Chevron Phillips Marlex® C513 High density polyethylene
(discontinued **)
Benefits: outstanding impact and creep resistance, outstanding ESCR, excellent processabilityApplications: intermediate bulk containers, agricultural containersInformation provided by Chevron Philli..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
|
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **)
Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
ExxonMobil HD 6908.18 Injection Molding Resin
(discontinued **)
HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stif..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
|
NOVA Chemicals Sclair® 14B3 Butene LMDPE Film Resin
(discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | Solenoid Brittle Point; ASTM D746 |
|
Kolon KOPEL® KP3363 General Purpose TPE Resin
KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Micropol Microstat ML21 Linear medium density static dissipative polyethylene
Information provided by Micropol Limited
|
|||
| Brittleness Temperature | -70.0 °C | -94.0 °F | ASTM D746 |
|
Lushan EP252 Adhesive Resin for Sewerage and Drainage Pipe
Adhesive resin Lushan EP252 is maleic grafted polyethylene. It’s mainly used for reinforced PE spiral corrugated steel pipes and steel wire with larger caliber. Adhesive resin Lushan EP252 solv..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Borealis Borecene Compact™ RM8346 Black Linear Polyethylene for Rotational Molding
Borecene Compact RM8346 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides ..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Borealis Borstar® HE3410 HDPE for Sewage Pipes
Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an ..
|
|||
| Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
|
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
|
Lubrizol ESTANE® T5192 Ether-Type Dissipative Compound (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
|
Toyobo A3064D Thermoplastic Polyurethane Elastomer, Injection Grade
Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information ..
|
|||
| Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
|
Lubrizol ESTANE® 58201 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
|
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
|
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
|
Lubrizol ESTANE® T5191 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Brittleness Temperature | >= -70.0 °C | >= -94.0 °F | ASTM D746 |
|
ExxonMobil LL 6407 Injection Molding Resin
(discontinued **)
LL 6100 is a narrow molecular weight butene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processability with minimal wa..
|
|||