| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glow Wire Test |
675
°C <br>@Thickness 3.20 mm
|
1250
°F <br>@Thickness 0.126 in
|
Glow Wire Ignition Temperature; IEC 695-2-13 |
|
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It ..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.800 - 3.00 mm
|
1250
°F <br>@Thickness 0.0315 - 0.118 in
|
Ignition Temperature; IEC 60695-2-13 |
|
PolyOne Bergamid™ A700 blue VN4817CF Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.750 mm
|
1250
°F <br>@Thickness 0.0295 in
|
IEC 60695-2-12 |
|
DuPont Performance Polymers Rynite® 415HP BK503 PET
(Unverified Data**)
Rynite® 415HP BK503 is a 15% glass reinforced modified polyethylene terephthalate with improved for easy, fast processing over a broad molding range with excellent balance of strength, stiffness, a..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
IEC 60695-2-12 |
|
DuPont Performance Polymers Rynite® 415HP BK503 PET
(Unverified Data**)
Rynite® 415HP BK503 is a 15% glass reinforced modified polyethylene terephthalate with improved for easy, fast processing over a broad molding range with excellent balance of strength, stiffness, a..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
Mitsubishi Xantar® C CM 206 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 3.00 mm
|
1250
°F <br>@Thickness 0.118 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
Mitsubishi Xantar® C CM 206 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
Mitsubishi Xantar® C CM 406 FD C CM 406 Polycarbonate/ABS Blend (European Grade)
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.800 mm
|
1250
°F <br>@Thickness 0.0315 in
|
ignition temperature; ISO 60695-2-12 |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY
Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.750 mm
|
1250
°F <br>@Thickness 0.0295 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 3.00 mm
|
1250
°F <br>@Thickness 0.118 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM
Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.750 mm
|
1250
°F <br>@Thickness 0.0295 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.750 mm
|
1250
°F <br>@Thickness 0.0295 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 3.00 mm
|
1250
°F <br>@Thickness 0.118 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.750 mm
|
1250
°F <br>@Thickness 0.0295 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.750 mm
|
1250
°F <br>@Thickness 0.0295 in
|
Fammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM
Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.750 mm
|
1250
°F <br>@Thickness 0.0295 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, ..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, ..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.750 mm
|
1250
°F <br>@Thickness 0.0295 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
DAM; Ignition Temp; IEC 60695-2-13 |
|
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 3.00 mm
|
1250
°F <br>@Thickness 0.118 in
|
Flame Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded
Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold ..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.750 mm
|
1250
°F <br>@Thickness 0.0295 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 3.00 mm
|
1250
°F <br>@Thickness 0.118 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 0.850 mm
|
1250
°F <br>@Thickness 0.0335 in
|
IEC 60695-2-12 |
|
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)
Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
IEC 60695-2-12 |
|
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)
Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a..
|
|||
| Glow Wire Test |
675
°C <br>@Thickness 1.50 mm
|
1250
°F <br>@Thickness 0.0591 in
|
IEC 60695-2-12 |
|
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&
Sorona® 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a..
|
|||