Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glow Wire Test = 1560 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Glow Wire Test 850 °C
<br>@Thickness 1.00 mm
1560 °F
<br>@Thickness 0.0394 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Lexan® 2014R PC (Europe-Africa-Middle East)
LEXAN 2014R is a medium viscosity flame retardant grade, This material contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region...
Glow Wire Test 850 °C
<br>@Thickness 0.800 mm
1560 °F
<br>@Thickness 0.0315 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Asia Pacific)
Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp..
Glow Wire Test 850 °C
<br>@Thickness 1.60 mm
1560 °F
<br>@Thickness 0.0630 in
Flammability Index; IEC 60695-2-12
PolyOne Bergamid™ B70 UF V2 Polyamide 6 (Nylon 6)
Information provided by PolyOne
Glow Wire Test 850 °C
<br>@Thickness 1.00 mm
1560 °F
<br>@Thickness 0.0394 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East)
LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A..
Glow Wire Test 850 °C
<br>@Thickness 2.00 mm
1560 °F
<br>@Thickness 0.0787 in
IEC 60695-2-12
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char..
Glow Wire Test 850 °C
<br>@Thickness 1.00 mm
1560 °F
<br>@Thickness 0.0394 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Lexan® ML3019 PC (Europe-Africa-Middle East)
LEXAN ML3019 is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications like industrial enclosures and fuse boxes requiring a low knock-out strength for..
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® FC 22 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® FC 23 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® G2F 23 UR Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C
<br>@Thickness 1.50 mm
1560 °F
<br>@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C
<br>@Thickness 1.50 mm
1560 °F
<br>@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® MX 1094 Polycarbonate-9% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C
<br>@Diameter 3.00 mm
1560 °F
<br>@Diameter 0.118 in
GWIT; IEC 60695-2-13
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
Glow Wire Test 850 °C
<br>@Thickness 1.00 mm
1560 °F
<br>@Thickness 0.0394 in
GWFI/GWT
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous freeAvailability: Africa & Middle East; Asia Pacific; Europe..
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi..
Glow Wire Test 850 °C
<br>@Thickness 2.00 mm
1560 °F
<br>@Thickness 0.0787 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 2400 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Glow Wire Test 850 °C
<br>@Thickness 1.00 mm
1560 °F
<br>@Thickness 0.0394 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Glow Wire Test 850 °C
<br>@Thickness 0.750 mm
1560 °F
<br>@Thickness 0.0295 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 2607 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Glow Wire Test 850 °C
<br>@Thickness 1.50 mm
1560 °F
<br>@Thickness 0.0591 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 3100 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Glow Wire Test 850 °C
<br>@Thickness 2.00 mm
1560 °F
<br>@Thickness 0.0787 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 3100 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
b.o. EDF HN60 E.02
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Glow Wire Test 850 °C
<br>@Thickness 1.00 mm
1560 °F
<br>@Thickness 0.0394 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
GWIT; IEC 60695-2-13
Covestro Makrolon® XT5010 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Easy processing• Low..
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
Glow-Wire Ignition; IEC 60695-2-13
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded
Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym..
Glow Wire Test 850 °C
<br>@Thickness 2.00 mm
1560 °F
<br>@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
Glow Wire Test 850 °C
<br>@Thickness 2.00 mm
1560 °F
<br>@Thickness 0.0787 in
GWFI; IEC 60695
Eurotec® Tecotek® PC30 NL RX PC, unfilled, improved flow & low temperature impact, natural
Information provided by Eurotec®
Glow Wire Test 850 °C
<br>@Thickness 1.50 mm
1560 °F
<br>@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
Glow Wire Test 850 °C
<br>@Thickness 3.00 mm
1560 °F
<br>@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® F 22 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
Glow Wire Test 850 °C
<br>@Thickness 1.00 mm
1560 °F
<br>@Thickness 0.0394 in
IEC 60695-2-12
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East)
VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes.