| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glow Wire Test |
960
°C <br>@Thickness 3.20 mm
|
1760
°F <br>@Thickness 0.126 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66
Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.60 mm
|
1760
°F <br>@Thickness 0.0630 in
|
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® 3413R PC (Europe-Africa-Middle East)
LEXAN 3413R is a high viscosity, 30% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance.
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 0.800 mm
|
1760
°F <br>@Thickness 0.0315 in
|
Flammability Index; IEC 60695-2-12 |
|
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.50 mm
|
1760
°F <br>@Thickness 0.0591 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 3.00 mm
|
1760
°F <br>@Thickness 0.118 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.50 mm
|
1760
°F <br>@Thickness 0.0591 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.50 mm
|
1760
°F <br>@Thickness 0.0591 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
Mitsubishi Xantar® MX 1000 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
960
°C <br>@Diameter 0.400 mm
|
1760
°F <br>@Diameter 0.0157 in
|
GWFI; IEC 60695-2-12 |
|
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 0.800 mm
|
1760
°F <br>@Thickness 0.0315 in
|
GWFI; IEC 60695-2-12 |
|
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 2.00 mm
|
1760
°F <br>@Thickness 0.0787 in
|
GWFI/GWT |
|
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.00 mm
|
1760
°F <br>@Thickness 0.0394 in
|
GWFI/GWT |
|
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 2.00 mm
|
1760
°F <br>@Thickness 0.0787 in
|
GWFI/GWT |
|
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin ..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 3.00 mm
|
1760
°F <br>@Thickness 0.118 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
Mitsubishi Xantar® C CF 107 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 3.00 mm
|
1760
°F <br>@Thickness 0.118 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
Mitsubishi Xantar® C CF 407 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.50 mm
|
1760
°F <br>@Thickness 0.0591 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
Mitsubishi Xantar® MX 1002 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 0.800 mm
|
1760
°F <br>@Thickness 0.0315 in
|
ISO 60695-2-12 |
|
Solvay TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY
Description: High flow Polyamide PA66 Flame retarded grade reinforced with 30% glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applicat..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 0.800 mm
|
1760
°F <br>@Thickness 0.0315 in
|
ISO 60695-2-12 |
|
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY
Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 0.800 mm
|
1760
°F <br>@Thickness 0.0315 in
|
ISO 60695-2-12 |
|
Solvay TECHNYL® C 52G1 V25 Grey R7035 (XC 1329/A) PA6, DRY
Description: Polyamide 6, Glass-filled, glow-wire modified, color stabilized, lubricated for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Application..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 2.00 mm
|
1760
°F <br>@Thickness 0.0787 in
|
GWFI; IEC 60695 |
|
Eurotec® Tecomid® NB30 GR15 BK005 FS90 PA6, 15% glass fiber reinforced, flame retardant - halogen & red phosphorus free, low smoke & toxic gas grade
Information provided by Eurotec®
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 2.00 mm
|
1760
°F <br>@Thickness 0.0787 in
|
GWFI; IEC 60695 |
|
Eurotec® Tecomid® NB40 GR30 NL AX70 PA6, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 0.750 mm
|
1760
°F <br>@Thickness 0.0295 in
|
Ignition Temperature; IEC 60695-2-13 |
|
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 3.00 mm
|
1760
°F <br>@Thickness 0.118 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.50 mm
|
1760
°F <br>@Thickness 0.0591 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 3.00 mm
|
1760
°F <br>@Thickness 0.118 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.00 mm
|
1760
°F <br>@Thickness 0.0394 in
|
IEC 695-2-1 |
|
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.50 mm
|
1760
°F <br>@Thickness 0.0591 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 2.00 mm
|
1760
°F <br>@Thickness 0.0787 in
|
GWFI/GWT |
|
LATI Laticonther 80 GR/50 PPS, 50% Graphite Reinforced
High thermal conductivity product based on Polyphenylene Sulfide (PPS). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 0.750 mm
|
1760
°F <br>@Thickness 0.0295 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 1.50 mm
|
1760
°F <br>@Thickness 0.0591 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Glow Wire Test |
960
°C <br>@Thickness 0.800 mm
|
1760
°F <br>@Thickness 0.0315 in
|
Flammability Index; DAM; IEC 60695-2-12 |
|
Solvay Technyl® A 402 H1 Nylon 66
Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit..
|
|||