| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East)
CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.00 mm
|
1200
°F <br>@Thickness 0.0394 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East)
Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by ..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 0.800 mm
|
1200
°F <br>@Thickness 0.0315 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66
Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 0.800 mm
|
1200
°F <br>@Thickness 0.0315 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 0.800 mm
|
1200
°F <br>@Thickness 0.0315 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66
Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 0.800 mm
|
1200
°F <br>@Thickness 0.0315 in
|
uncolored material; Ignition Temperature; IEC 60695-2-13 |
|
PolyOne Bergamid™ A700 Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66
Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66
Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 0.800 mm
|
1200
°F <br>@Thickness 0.0315 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 0.800 mm
|
1200
°F <br>@Thickness 0.0315 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A3 H ZB High Impact PA66
Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas ..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 0.800 mm
|
1200
°F <br>@Thickness 0.0315 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 0.800 mm
|
1200
°F <br>@Thickness 0.0315 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 0.800 mm
|
1200
°F <br>@Thickness 0.0315 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66
Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66
Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.50 mm
|
1200
°F <br>@Thickness 0.0591 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific)
DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.60 mm
|
1200
°F <br>@Thickness 0.0630 in
|
ignition temperature; ISO 60695-2-13 |
|
Solvay TECHNYL® B 50 H1 PA66/6, DRY
Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
Ignition Temperature; ISO 60695-2-13 |
|
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY
Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent ..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.60 mm
|
1200
°F <br>@Thickness 0.0630 in
|
ISO 60695-2-12 |
|
Solvay TECHNYL® A 217 PA66, DRY
Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.60 mm
|
1200
°F <br>@Thickness 0.0630 in
|
Ignition Temperature; ISO 60695-2-13 |
|
Solvay TECHNYL® A 217 PA66, DRY
Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.60 mm
|
1200
°F <br>@Thickness 0.0630 in
|
ISO 60695-2-12 |
|
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY
Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
Ignition Temperature; ISO 60695-2-13 |
|
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is ..
|
|||
| Glow Wire Test |
650
-
750
°C <br>@Thickness 2.00 mm
|
1200
-
1380
°F <br>@Thickness 0.0787 in
|
VDE 0471/P2-4, IEC 695 |
|
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS |
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
VDE 0471/P2-4, IEC 695 |
|
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene |
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
VDE 0471/P2-4, IEC 695 |
|
EPICHEM Epilac ABS-BLACK Acrylonitrile Butadiene Styrene |
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
VDE 0471/P2-4, IEC 695 |
|
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber
Characteristics: 17% glass fibre filled
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
VDE 0471/P2-4, IEC 695 |
|
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
Glow-Wire Ignition; IEC 60695-2-13 |
|
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.00 mm
|
1200
°F <br>@Thickness 0.118 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.00 mm
|
1200
°F <br>@Thickness 0.118 in
|
IEC 60695-2-12 |
|
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)
Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont..
|
|||