| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glow Wire Test |
850
°C <br>@Thickness 0.800 mm
|
1560
°F <br>@Thickness 0.0315 in
|
Glow Wire Flammability Index; IEC 694-2-12 |
|
Nilit Nilitop BT N Unfilled, Nucleated PBT
Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.00 mm
|
1560
°F <br>@Thickness 0.0394 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East)
LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.00 mm
|
1560
°F <br>@Thickness 0.0394 in
|
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® 500 PC (Europe-Africa-Middle East)
LEXAN 500 resin grade is a medium viscosity, 10% glass reinforced, flame retardant product designed for applications requiring high rigidity together with high heat resistance and excellent impact p..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 3.00 mm
|
1560
°F <br>@Thickness 0.118 in
|
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Europe-Africa-Middle East)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.00 mm
|
1560
°F <br>@Thickness 0.0394 in
|
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® ML3290 PC (Europe-Africa-Middle East)
LEXAN ML3290 is a high viscosity flame retardant UV stabilized grade especially developed for the extrusion of complex sheet and profiles. LEXAN ML3290 is used in applications where a combination of..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 2.00 mm
|
1560
°F <br>@Thickness 0.0787 in
|
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.00 mm
|
1560
°F <br>@Thickness 0.0394 in
|
IEC 60695-2-12 |
|
SABIC Innovative Plastics Lexan® 950A PC (Europe-Africa-Middle East)
LEXAN 950A is a high viscosity flame retardant grade, especially suitable for electrical applications.
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 0.800 mm
|
1560
°F <br>@Thickness 0.0315 in
|
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 3.00 mm
|
1560
°F <br>@Thickness 0.118 in
|
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 3.00 mm
|
1560
°F <br>@Thickness 0.118 in
|
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
|
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 3.00 mm
|
1560
°F <br>@Thickness 0.118 in
|
Glow Wire Ignition Temperature; IEC 60695-2-13 |
|
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 3.00 mm
|
1560
°F <br>@Thickness 0.118 in
|
Glow Wire Ignition Temperature; IEC 60695-2-13 |
|
Mitsubishi Xantar® FC 19 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.50 mm
|
1560
°F <br>@Thickness 0.0591 in
|
Glow Wire Ignition Temperature; IEC 60695-2-13 |
|
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.50 mm
|
1560
°F <br>@Thickness 0.0591 in
|
Glow Wire Ignition Temperature; IEC 60695-2-13 |
|
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
850
°C <br>@Diameter 0.400 mm
|
1560
°F <br>@Diameter 0.0157 in
|
GWIT; IEC 60695-2-13 |
|
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Glow Wire Test |
850
°C <br>@Diameter 3.00 mm
|
1560
°F <br>@Diameter 0.118 in
|
GWIT; IEC 60695-2-13 |
|
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.50 mm
|
1560
°F <br>@Thickness 0.0591 in
|
Glow Wire Ignition Temperature; IEC 60695-2-13 |
|
Mitsubishi Xantar® MX 1082 Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 3.00 mm
|
1560
°F <br>@Thickness 0.118 in
|
Glow Wire Ignition Temperature; IEC 60695-2-13 |
|
Mitsubishi Xantar® MX 2015 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.00 mm
|
1560
°F <br>@Thickness 0.0394 in
|
GWIT |
|
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant
Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 4.00 mm
|
1560
°F <br>@Thickness 0.157 in
|
GWIT; IEC 60695-2-13 |
|
Covestro Makrolon® 2405 MAS057 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 0.750 mm
|
1560
°F <br>@Thickness 0.0295 in
|
GWFI; IEC 60695-2-12 |
|
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 0.750 mm
|
1560
°F <br>@Thickness 0.0295 in
|
GWFI; IEC 60695-2-12 |
|
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.50 mm
|
1560
°F <br>@Thickness 0.0591 in
|
GWFI; IEC 60695-2-12 |
|
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 3.00 mm
|
1560
°F <br>@Thickness 0.118 in
|
b.o. EDF HN60 E.02 |
|
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.00 mm
|
1560
°F <br>@Thickness 0.0394 in
|
GWFI; IEC 60695-2-12 |
|
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.00 mm
|
1560
°F <br>@Thickness 0.0394 in
|
Glow-Wire Ignition; IEC 60695-2-13 |
|
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded
Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 2.00 mm
|
1560
°F <br>@Thickness 0.0787 in
|
GWIT; IEC 60695 |
|
Eurotec® Tecomid® NB30 GR15 BK005 FS90 PA6, 15% glass fiber reinforced, flame retardant - halogen & red phosphorus free, low smoke & toxic gas grade
Information provided by Eurotec®
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 2.00 mm
|
1560
°F <br>@Thickness 0.0787 in
|
GWFI; IEC 60695 |
|
Eurotec® Tecotek® PC30 NL RX PC, unfilled, improved flow & low temperature impact, natural
Information provided by Eurotec®
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 0.710 mm
|
1560
°F <br>@Thickness 0.0280 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
|
|||
| Glow Wire Test |
850
°C <br>@Thickness 1.50 mm
|
1560
°F <br>@Thickness 0.0591 in
|
Flammability Index; IEC 60695-2-12 |
|
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM