Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige
Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ISO 75.1
Solvay Engineered Polymers DEXFLEX® E756 TPO  (discontinued **)
Description: DEXFLEX® E756 thermoplastic olefinic elastomer (TPO) is designed for extruded automotive air-bag covers. This material provides excellent rigidity, durability and low-temperature toug..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil LL 8450 Rotational Molding Resin  (discontinued **)
LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil LL 8455.24 Rotational Molding Resin  (discontinued **)
LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil LLP8455.24 Rotational Molding Resin  (discontinued **)
LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic  (discontinued **)
Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil HD 6714.17 Injection Molding Resin  (discontinued **)
HD 6714 is a narrow molecular weight hexene copolymer designed for outstanding processability to maximize injection molding productivity. This resin is ideally suited for thin wall multicavity part..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
NOVA Chemicals Novapol® TR-0338-UI Hexene MDPE Rotational Molding Resin
Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, ..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
NOVA Chemicals Novapol® TR-0338-UIG Hexene MDPE Rotational Molding Resin
Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, ..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
LyondellBasell Lupolen® 3821 D MDPE
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
Lucent Polymers TPO-1015 Thermoplastic Polyolefin
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C

@Thickness 3.20 mm
100 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil HD 6719.17 Injection Molding Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil HD 6719.62 Injection Molding Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil LL 8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil LL 8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LL 8450.31 Linear Low Density Polyethylene Resin
Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil LLP8450.31 Rotational Molding Resin
LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil LLP8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil LLP8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ASTM D648
Clariant 6008 L Nylon 6, High Impact, Injection Molding
Data provided by Clariant Masterbatches
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
ExxonMobil HD 6733.17 Injection Molding Resin
Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable ..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 - 55.0 °C
100 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 - 101 °C
100 - 214 °F
Average value: 67.4 °C Grade Count:4
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 - 55.0 °C
100 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Deflection Temperature at 1.8 MPa (264 psi) 37.8 - 125 °C
100 - 257 °F
Average value: 61.7 °C Grade Count:22
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..