| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 76.7 - 170 °C | 170 - 338 °F | Average value: 110 °C Grade Count:49 |
|
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 140 - 170 °C | 284 - 338 °F | Injection; ISO 75-A |
|
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 140 - 170 °C | 284 - 338 °F | Injection; ISO 75-A |
|
Raschig Group RALUPOL® 8602 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 - 170 °C | 149 - 338 °F | Average value: 100 °C Grade Count:3 |
|
Overview of materials for Nylon 12, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 47.0 - 170 °C | 117 - 338 °F | Average value: 101 °C Grade Count:7 |
|
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 150 - 170 °C | 302 - 338 °F | ISO 75 Af |
|
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
|
|||