| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | 120°C/h; ISO 75/1 |
|
Polykemi AB POLYshine PBT D201 FB60 PBT, Reinforced
Information provided by Polykemi AB
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | 120°C/h; ISO 75/1 |
|
Polykemi AB SCANMID 6 B22^ E F30 Nylon 6, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
190
°C <br>@Thickness 6.40 mm
|
374
°F <br>@Thickness 0.252 in
|
Unannealed; ASTM D648 |
|
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ISO 75 |
|
GEHR Plastics PEI Polyetherimide
Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and creep resistance. Its unique torque strength permits the economic..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
190
°C <br>@Thickness 6.40 mm
|
374
°F <br>@Thickness 0.252 in
|
Unannealed; ASTM D648 |
|
LG Chemical Lupox® SG5150 PBT+PET+GF15%
Description: Injection Molding, PBT+PET+GF15%, Good SurfaceApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | DIN 53461; ASTM D648 |
|
Kolon KOPA® KN135HB40SIBL Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ISO 75-1/-2 |
|
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
|
SABIC Innovative Plastics ULTEM 1010K PEI
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
190
°C <br>@Thickness 6.40 mm
|
374
°F <br>@Thickness 0.252 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
190
°C <br>@Thickness 6.40 mm
|
374
°F <br>@Thickness 0.252 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics ULTEM AUT195 PEI+PCE
High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method).
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
|
SABIC Innovative Plastics ULTEM DH1004 PEI |
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
190
°C <br>@Thickness 3.20 mm
|
374
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
190
°C <br>@Thickness 6.40 mm
|
374
°F <br>@Thickness 0.252 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific)
15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
190
°C <br>@Thickness 3.20 mm
|
374
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
190
°C <br>@Thickness 6.40 mm
|
374
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled
Information provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
|
SABIC Innovative Plastics Ultem 1010KM PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ASTM D648 |
|
Plenco 4327 Phenolic, Granular, Compression Molded
PLENCO 04327 is a heat resistant mineral filled phenolic molding compound offering excellent cosmetic characteristics and improved heat resistant properties. PLENCO 04327 is not intended for electri..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | dry; ISO 75-1/-2 |
|
DSM Stanyl® TS300 PA46 |
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ISO 75-1/-2 |
|
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | dry; ISO 75-1/-2 |
|
DSM Stanyl® TW341-B PA46
Heat Stabilized, Lubricated
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ISO 75 |
|
BASF Petra® 7010 BK 5830 15% Glass Filled PET
Description: Petra 7010 BK5830 is a 15% glass fiber reinforced, pigmented black injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ASTM D648 |
|
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound
ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ISO R75 |
|
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ISO 179 |
|
CP-Polymer-Technik Wellamid® 6000 CF 10 HWCP 10% Carbon Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP STAT-KON PX05047 PA 6 (Europe-Africa-Middle East)
LNP* Stat-kon* PX05047 is a compound based on PA 6 resin containing Carbon Fiber, Proprietary Filler (s). Added features include: Electrically Conductive, High Impact.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
190
°C <br>@Thickness 3.20 mm
|
374
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ISO 75-2 |
|
CENTROPLAST CENTRO HPM Polyetherimide
This material has high strength and rigidity at high temperatures, with good electrical properties. Applications include electrical insulators, and load-bearing components.Information provided by C..
|
|||