| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | STN EN ISO 75/A |
|
Plastcom SLOVAMID 6 SGF 30 Polyamide 6, 30% Milled Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 30% of milled glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consum..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | 120°C/h; ISO 75/1 |
|
Polykemi AB SCANMID 6 B11^ F30 FR5 Nylon 6, Glass Fiber Reinforced, Flame Retardant
Information provided by Polykemi AB
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | Annealed; ISO 75-2/A |
|
PolyOne Nymax™ X GMF 604 40 UV Black 148 rev 4 Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
|
DSM Akulon® K224-TPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry)
(discontinued **)&l
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
195
°C <br>@Thickness 6.40 mm
|
383
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
LG Chemical LUCON PO6062 mPPO+CNT+CF+GF
Description: Injection Molding, mPPO+CNT+CF+GF, High Strength, Heat StabilityApplication: ATM parts, LCD Cell TrayCAS No. 35134-01-4, 25038-54-4, 65997-17-3, 7440-44-0 and 7782-42-5Information provi..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-1, -2 |
|
Lanxess Pocan® ECO T 3220 000000 PBT + PET, 20% Glass Fiber
PBT + PET, 20% glass fibers, injection molding, improved surface finish, contains 28% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | DIN 53461; ASTM D648 |
|
Kolon KOPA® KN178MT40 M/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
|
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-1,-2 |
|
Lanxess Durethan® BKY 115 H3.0 DUS008 Nylon 6, 15% Glass Fiber
PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | |
|
Lehmann & Voss LUVOCOM® 1100-7721/WT9016 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP STAT-KON PFD04 PA 6
LNP* STAT-KON* PFD04 is a compound based on Nylon 6 containing 20% Glass Fiber. Added feature of this grade is: Ellectrically Conductive.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS
LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
195
°C <br>@Thickness 3.20 mm
|
383
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 (Asia Pacific)
LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP Thermocomp 9X04488 POLYPHENYLENESULFONE
LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-93 |
|
Wellman EcoLon® MRGF1518-BK3 38% Mineral/Glass Reinforced Post Consumer Compound Nylon 66
Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 66Information provided by Wellman.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
|
DSM Akulon® F249-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
|
DSM Akulon® K223-HGM24 Nylon 6-30% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
|
EMS-Grivory Grivory® BG-15 PA6-GF15
Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Ae |
|
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75 |
|
Eurotec® Tecomid® NB40 GR30 NL IM PA6, 30% glass fiber reinforced, impact modified, natural
Information provided by Eurotec®
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
|
Eurostar Starflam PF0069 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PF0069 is a Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ASTM D648 |
|
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin
30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ASTM D648 |
|
Beijing Ranger Chem PBT-201-G15 291 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | dry; ISO 75 |
|
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced
20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-1/2 |
|
Eurotec® Tecomid® NB40 GR30 NL IH PA 6 30% glass fiber reinforced, impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | As Molded; ASTM D648A |
|
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac
FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | compression molded annealed; ASTM D-648-95 |
|
Multibase Multi-ABS 2945 FR Flame Retardant ABS
Data provided by Multibase.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
|
DSM Arnite® TV4 230 PBT-15% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||