Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 23.9 °C
75.0 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA11
Availability: North AmericaForms: PelletsFeatures: Medium ViscosityTPCI# 6486106Information provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 23.9 °C
75.0 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA11 GB7 HS L 7% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 7% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by T..
Deflection Temperature at 1.8 MPa (264 psi) 23.9 °C
75.0 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA11 GL8 HS UV
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Graphite Powder Lubricant and UV StabilizerFeatures: Heat Stabilized. Good UV Resistance and LubricatedAppearance: Natural ColorIn..