| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Unannealed; ISO 75-2/A |
|
PolyOne OnForce™ LFT NN-50LGF/000 HS Natural Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | STN EN ISO 75-2 (A) |
|
Plastcom SLOVAMID® 6 NG1 GF 30 HLS PA6 reinforced with glass fiber, UV stabilized, hydrolysis resistant
PA 6 for injection molding, reinforced with 30% glass fiber, for moldings used in the automotive, weather and UV stabilized. Determined for using in outside automotive applications like door handle,..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75/A |
|
Grupo Repol Dinalon® A1S25 G50 PA66 50% Glass Fiber
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | |
|
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | |
|
LATI Latilub 57D-15T G/30 PPA, 30% Glass Fiber Reinforced
Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75/Af |
|
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75/Af |
|
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, DRY
Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: EuropeProduct Applications: TECHNYL A 218W V3..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
255
°C <br>@Thickness 3.20 mm
|
491
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 (Asia Pacific)
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GF43 HS L BK001 43% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | GB/T 1634.2-2004 |
|
Sichuan Deyang Haton® hGR505 Polyphenylene Sulfide/PA Alloy
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | GB/T 1634.2-2004 |
|
Sichuan Deyang Haton® hGR515 Polyphenylene Sulfide/PA Alloy
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
255
°C <br>@Thickness 3.20 mm
|
491
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66
LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
255
°C <br>@Thickness 3.20 mm
|
491
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific)
LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ASTM D648 |
|
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY
Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75/Af |
|
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-1/-2 |
|
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30
Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-1/-2 |
|
EMS-Grivory Grivory® GVL-6H nat PA*-GF60
Product description: Grivory GVL-6H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H na..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | DAM; ISO 75-1/-2 |
|
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75 |
|
Eurotec® Tecomid® NA40 GR30 NL HS PA6.6, 30% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-1/2 |
|
Eurotec® Tecomid® NA40 GR30 NL RT PA 6.6 30% glass fiber reinforced, very low friction and wear
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75 |
|
Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-1/-2 |
|
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60
Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-1/2 |
|
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75 |
|
BASF Ultramid® N-333 NF3001 33% Glass Filled PA66 (Dry)
Ultramid N-333 NF3001 is a 33% glass reinforced, heat stabilized, injection molding
PA66 uncolored.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | HDT/A; ISO 75-2 |
|
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75 |
|
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry)
Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75/Af |
|
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits:..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ASTM-D648 |
|
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber
A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
|
|||