Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 265 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
ISO 75-1/-2
Kuraray Genestarâ„¢ GC1201A-M41 Nylon, Glass Filled and Carbon Filled
Reinforced injection grade for conductive applications.Main Features:ConductivityHeat resistanceChemical resistanceExample of applications:Quick connector
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Lehmann & Voss LUVOCOM® 1301-7869/BL PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C

@Thickness 3.20 mm
509 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear ..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C

@Thickness 3.20 mm
509 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding.
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
GB/T 1634.2-2004
Sichuan Deyang Haton® hGR302 PPS / F4 Polyphenylene Sulfide
Injection molding, anti-frictionInformation provided by Sichuan Deyang Chemical Co., LTD
Deflection Temperature at 1.8 MPa (264 psi) 265 °C

@Thickness 3.20 mm
509 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear
LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
ISO 75-1/-2
Barlog Plastics KEBATRON C2065X3 PPS, cross-linked, 65% glass fiber / mineral reinforced, reduced residual chlorine
PPS-GF/MD 65Information provided by BARLOG plastics GmbH.
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Unannealed; ASTM D648
LNP Lubricomp® OCL-4534 EM Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant  (discont
Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
LATI Latilub 80-15T G/30 PPS, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..