Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 277 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
Ovation Polymers Nemcon™ H PC DP105/X3 BK Polycarbonate
Polycarbonate-Black colored, thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Treatment Temp. 120 °C,
Time 7200 sec
277 °F

@Treatment Temp. 248 °F,
Time 2.00 hour
annealed; ISO 75/Ae
SABIC Innovative Plastics Lexan® 3441R PC (Europe-Africa-Middle East)
Lexan 3441R is a medium viscosity, 10% glass reinforced polycarbonate grade, compliant with European food contact regulation EC Directive 2002/72/EC. The grade is especially designed for application..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® 500ECR PC (Asia Pacific)
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Annealed 120°C, 2hrs; ISO 75/Ae
SABIC Innovative Plastics Lexan® 503R PC (Europe-Africa-Middle East)
LEXAN 503R is a medium viscosity, 10% glass reinforced, UV-stabilized, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and exce..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics Lexan® 505R PC
Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm...
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific)
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC
LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP DF0069P PC
LNP THERMOCOMP* DF0069P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC
LNP THERMOCOMP* DF006ER is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC
LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific)
Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
ASTM D648
Samyang Trirex® 3027PJ Polycarbonate
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PJ is an extrusion grade.Information provided by Samyang.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
annealed; ASTM D648
Styron CALIBREâ„¢ IM 401-18 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS
LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS resin containing 30% Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA
NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Stat-kon DE0049 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DC-1004 FR is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.This..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC
LNP THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding. Mold Release
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP DF008ERH PC
LNP THERMOCOMP* DF008ERH is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
0.125 in, 8000 ipm, annealed; ASTM D648
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate
EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
ASTM D648
Zeon Chemicals Zeonex® 690R Cyclo-Olefin Polymer
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Plain Cast Resin; ASTM D648
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
ISO 75-1/-2
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
ASTM D648
E-Polymers TEKAPPO® J920 20% Glass Fiber Reinforced M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Aclo Accutech Polypropylene Homopolymer HP0336G25M5CL Glass/Mineral Reinforced Coupled
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
ISO 75
Arkema Group Rilsan® Clear G170 Polyamide
Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
ASTM D648
A. Schulman ComAlloy Voloy® 112 Polypropylene, Glass Reinforced, Chemically Coupled, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Thermocomp MF0069S PP
LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Verton NV006E PC/ABS
LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas region..