Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Resinoid 1365 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Deflection Temperature at 1.8 MPa (264 psi) >= 315 °C
>= 599 °F
ASTM D648
Resinoid 1382 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ISO 75
Gharda Chemicals GATONE™ PEEK, 30% Glass Reinforced  (discontinued **)
GATONE™ PEEK grades with glass fiber reinforcements ranging from 10- 40 % are available in natural or desired colors. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ISO 75
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced  (discontinued **)
GATONE™ PEEK grades with carbon fiber reinforcements ranging from 10- 40 % are available in natural or desired color. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Gharda Chemicals GATONE™ 5630GF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Gharda Chemicals GATONE™ 5630CF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Gharda Chemicals GATONE™ 5330FC Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Annealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Annealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ISO 75-f
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Lehmann & Voss LUVOCOM® 1105-8317/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Lehmann & Voss LUVOCOM® 1105/GF/30/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Lehmann & Voss LUVOCOM® 1105-0895/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Lehmann & Voss LUVOCOM® 1105-7128 PEEK, with glass fiber, low-warpage
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Not flammable.High continuos use temperature.High..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Lehmann & Voss LUVOCOM® 1105-8389/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Lehmann & Voss LUVOCOM® 1105-8402 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ISO 75
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber
Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical ..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Annealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Annealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Annealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Gharda Chemicals GATONE™ 5330GF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Gharda Chemicals GATONE™ 5330CF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Resinoid 1324 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Resinoid 1329 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Lehmann & Voss LUVOCOM® 1105-7173/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ISO 75A-f
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..