Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 320 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Plastcom SLOVALEN PH 69 GF 45 PP, 45% glass fibre
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 45% glass fibre, contains the modifier of mechanical properties.Thermo stable. Increased strength in comparison wit..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-1/-2
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data)
Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black..
Deflection Temperature at 1.8 MPa (264 psi) 160 - 180 °C
320 - 356 °F
ISO 75-A
Raschig Group DECAL® 2061 Phenolic
Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and ..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Unannealed; ISO 75-2/A
PolyOne Bergamid™ B650 Mi10 Polyamide 6 (Nylon 6)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Unannealed; ISO 75-2/A
PolyOne Bergamid™ B650 Mi10 Polyamide 6 (Nylon 6)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 160 - 368 °C
320 - 694 °F
Average value: 287 °C Grade Count:17
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
<br>@Thickness 6.40 mm
320 °F
<br>@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity
Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Asia Pacific)
LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP VERTON MV008S PP (Europe-Africa-Middle East)
LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
<br>@Thickness 6.40 mm
320 °F
<br>@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific)
PPO/PS unfilled high heat
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
<br>@Thickness 3.20 mm
320 °F
<br>@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA4/6 GF5 IM HS BK 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifie..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP VERTON MV00ASXP PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-2
Borealis Nepol™ GB303HP 30% Long Glass Fiber Reinforced Polypropylene
Nepol GB303HP is a 30% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive)
Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 32..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-3 ESD PA12-GF30
Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Ensinger Tecapeek® MT Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Azdel Plus C467-B01 45% Chopped Fiber Mat / PP Resin Matrix (Mineral filled)
AZDEL® C467-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Aclo Accutech Polypropylene Homopolymer HP0336G40CL Glass Reinforced Coupled
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Unitika P-3001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Unannealed, 0.125 in bars; ASTM D648
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled &nbsp;(discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
<br>@Temperature 200 °C,<br> Time 14400 sec
320 °F
<br>@Temperature 392 °F,<br> Time 4.00 hour
ISO 75-f
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..