| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 194 - 256 °C | 381 - 493 °F | Average value: 232 °C Grade Count:7 |
|
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP LUBRICOMP ICL34 PA6.12
LNP* LUBRICOMP* ICL34 is a compound based on Nylon 6/12 containing 20% Carbon Fiber, 15% PTFE. Added features include: Wear Resistant.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP STAT-KON WE003ER PBT (Europe-Africa-Middle East)
LNP* Stat-kon* WE003ER is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Easy Molding, Easy Release, Electrically Conductive.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
194
°C <br>@Thickness 3.20 mm
|
381
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific)
Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP THERMOCOMP EX06430H PEI
LNP* THERMOCOMP* EX06430H is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this grade is: Healthcare.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
194
°C <br>@Thickness 6.40 mm
|
381
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
194
°C <br>@Thickness 3.20 mm
|
381
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics LNP Thermocomp OF003A PPS
LNP* Thermocomp* OF003A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 (Europe-Africa-Middle East)
LNP* THERMOCOMP* QF0069 is a compound based on PA610 resin contaning Glass Fiber, Flame Retardant. Added features include: Flame retardant.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
194
°C <br>@Thickness 3.20 mm
|
381
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOCOMP WF0039U PBT
LNP* THERMOCOMP* WF0039U is a compound based on PBT resin containing 15% Glass Fiber. Added features of this grade include: Flame Retardant and UV Stabilized.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
194
°C <br>@Thickness 3.20 mm
|
381
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics LNP Thermocomp OF003A PPS (Asia Pacific)
LNP* Thermocomp* OF003A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
194
°C <br>@Thickness 6.40 mm
|
381
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | ASTM D648 |
|
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | ASTM D648 |
|
Plenco 2369 Phenolic, Granular, Compression Molded
PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | ASTM D648 |
|
Plenco 3509 Phenolic, Granular, Compression Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | ASTM D648 |
|
Plenco 4300 Phenolic, Granular, Transfer Molded
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | dry; ISO 75-1/-2 |
|
DSM Novamid® 1013G15 1 NA PA6-GF15
15% Glass Reinforced, Injection Molding
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | dry; ISO 75-1/-2 |
|
DSM Novamid® 1013GH15 1 NA/BK37 PA6-GF15
15% Glass Reinforced, Heat Stabilized, Injection Molding
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | ASTM D648 |
|
A. Schulman ComAlloy Lubrilon® 628 Nylon 6/6, Glass Fiber/Molybdenum Disulfide Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 - 260 °C | 381 - 500 °F | Average value: 246 °C Grade Count:35 |
|
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 194 °C | 381 °F | ASTM D648 |
|
Plenco 6527 Phenolic, Granular, Injection Molded
PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco.
|
|||