Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 523 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
523 °F
ASTM D648
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded &nbsp
AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d..
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
<br>@Thickness 3.20 mm
523 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP UFL269SA PPA
LNP* Lubricomp* UFL269SA is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Heat Stabilized,..
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
<br>@Thickness 3.20 mm
523 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP UFL269SA PPA (Asia Pacific)
LNP* Lubricomp* UFL269SA is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Heat Stabilized,..
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
523 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA
LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
523 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP UX05051 PPA (Europe-Africa-Middle East)
Internally lubricated Polyphthalamide compound, containing Glass Fiber and PTFE. Added features include Heat Stabilized, Flame Retardant and Hot Water Moldable
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
523 °F
ASTM D648
Plenco 08122 Polyester BMC, Compression Molded
PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
523 °F
ASTM D648
Plenco 08225 Polyester BMC, Compression Molded
PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding propert..
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
523 °F
ASTM D648
Plenco 08235 Polyester BMC, Compression Molded
PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable ..
Copyright © lookpolymers.com All Rights Reserved