| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | ASTM D648 |
|
Resinoid 1365 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | >= 315 °C | >= 599 °F | ASTM D648 |
|
Resinoid 1382 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | ISO 75 |
|
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced
(discontinued **)
GATONE™ PEEK grades with carbon fiber reinforcements ranging from 10- 40 % are available in natural or desired color. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | ASTM D648 |
|
Gharda Chemicals GATONE™ 5630CF Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | ASTM D648 |
|
Gharda Chemicals GATONE™ 5330FC Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | ASTM D648 |
|
Gharda Chemicals GATONE™ 5630FC Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | Annealed; ASTM D648 |
|
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | Annealed; ASTM D648 |
|
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | Annealed; ASTM D648 |
|
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | ISO 75-f |
|
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7920/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8317/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105/GF/30/TF/15 PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0706 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0895/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0918/EM/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7128 PEEK, with glass fiber, low-warpage
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Not flammable.High continuos use temperature.High..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8389/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7980 PEEK, with carbon fiber
Applications: medical engineeringHigh-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flamm..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0918/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | Annealed; ASTM D648 |
|
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | Annealed; ASTM D648 |
|
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | Annealed; ASTM D648 |
|
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | >= 315 °C | >= 599 °F | ASTM D648 |
|
Resinoid 1323 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | ASTM D648 |
|
Resinoid 1329 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °C | 599 °F | ISO 75A-f |
|
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..
|
|||