| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | Unannealed; ASTM D648 |
|
Multibase Nylex™ 2185 HFX Natural Polyamide + PP
Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | Unannealed; ASTM Data |
|
Americas Styrenics Styron® 666D Polystyrene
(discontinued **)
STYRON® 666D general purpose polystyrene resin is used in injection molding applications, particularly for medical, pharmaceutical and food uses. It offers excellent clarity, intermediate flow char..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | Unannealed; ISO 75A-1, -2 |
|
LyondellBasell Hostacomâ„¢ CB271FC Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB271FC high melt flow, 2,400 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® ASA 814 GY
Availability: North AmericaForms: PelletsFeatures: Good Weather ResistanceAppearance: GrayInformation provided by TP Composites, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
77.2
°C @Thickness 3.20 mm |
171
°F @Thickness 0.126 in |
Unannealed, Injection Molded; ASTM D648 |
|
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 3500 Natural 1050
Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 3501
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 3501 Natural 1050
Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 3501E
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 3501E Natural 1050
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 3502
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 3502E
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 4500R
Description: Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 4502
Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 7502
Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 7600B
Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | ASTM D648 |
|
Clariant Renol CAB1000 Cellulose Acetate Butyrate
Data provided by Clariant Masterbatches
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 3501 HF
Description: High FlowInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 7501
Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | |
|
Aclo Accucomp ABS ABS802L High Impact Grade |
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | |
|
Aclo Accucomp ABS ABS856BL High Flow Medium Impact Grade |
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | |
|
Aclo Accutech Polypropylene Homopolymer HP0334M40L Mica Reinforced |
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | |
|
Aclo Accutech Polypropylene Homopolymer HP0339W30L1 Wollastonite Reinforced |
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | ASTM D648 |
|
Americas Styrenics EC6600 High Impact Polystyrene
Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toy..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | unannealed; injection molded; ASTM D648 |
|
Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin
STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | |
|
Aclo Accutech Polypropylene Homopolymer HP0339W30L Wollastonite Reinforced |
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | ASTM D648 |
|
Americas Styrenics MC3700 High Heat Crystal Polystyrene
Product CharacteristicsEasy filling of thin-walled partsExceptional mold releaseImproved cycle times in hard to fill partsFood Contact CompliantUL Classification 94HBUSP Class VITypical Applications..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | |
|
Aclo Accucomp ABS ABS803L Medium Impact Grade |
|||