| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | |
|
Plastcom SLOVASTER® C FRU 2 PBT, flame retarder
FeaturesPC with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other hole products. Application in engineer..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ASTM D648 |
|
Shell Carilon® DA6P2L10 Polyketone, High Performance Lubricated Injection Molding Grade
(discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6P2L10 is a high-performance lubricated injection molding grade with mechanical properties which ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ISO 75A |
|
Lucite International Diakon® Rapide CLG 356B Enhanced Molding Acrylic Polymer
Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | |
|
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber
Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
96.0
°C <br>@Thickness 3.20 mm
|
205
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics LNP Lubricomp OP005XXC PPS
LNP LUBRICOMP* OP005XXC is a compound based on Polyphenylene Sulfide resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | |
|
Spartech Royalite R84 Proprietary Polymer Weather Resistant Sheet
Data provided by the manufacturer.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ISO 75-1/-2 |
|
Styrolution Luran® S 776 S Colored ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ISO 75 |
|
Styrolution Novodur® M201AS ABS
Novodur M201AS is a medium impact, high gloss injection molding grade with improved chemical resistanceInformation provided by Styrolution
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ISO 75 |
|
Styrolution Terluran® HI-10 ABS
Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ISO 75 |
|
Styrolution Terluran® SP-6 ABS
Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | unannealed; ISO 75 A |
|
Styron Pulse® A20-95 PC/ABS
A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | DIN 53461 |
|
Polyram RamLloy PJ701 ABS/ASA, General Purpose
PJ 701 IS A GENERAL PURPOSE INJECTION MOLDING ASA& ABS ALLOY . IT HAS GOOD MECHANICAL PROPERTIES SIMILAR TO ABS AND MUCH BETTER WEATHER RESISTANCE. AN IDEAL ECONOMIC CHOICE.Information provided ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ISO 75 |
|
Polyram RamLloy PJ702 ASA & ABS Alloy
A general purpose injection molding ASA & ABS alloy. It has good mechanical properties similar to ABS with much better weather resistance.Information provided by Polyram.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ISO 75 |
|
Polyram RamShine PAS702 ASA, UV Stabilized
UV stabilized, general purpose, injection molding ASA.Information provided by Polyram.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | annealed; ISO 75 |
|
Chi Mei Polylac® PA-746H ABS - High Flow
Super high flow, medium impact
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | annealed; ISO 75 |
|
Chi Mei Polylac® PA-747S ABS - Extrusion
High Impact Extrusion
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | annealed; ISO 75 |
|
Chi Mei Polylac® PA-763 ABS - Flame Retardant
F.R. High Heat Weather Resistant
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | annealed; ISO 75 |
|
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
High FDI; high heat
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ASTM D648 |
|
Ashley Polymers Ashlene® ABS Resin 223
Medium impact, medium flow, matte finish. Suitable for general purpose injection molding.Data provided by the manufacturer
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
96.0
°C <br>@Thickness 6.40 mm
|
205
°F <br>@Thickness 0.252 in
|
Method A; ASTM D648 |
|
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade
High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | Method A - Annealed; ASTM D-648 |
|
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ISO.75 DIN.53461 |
|
Omnia Plastica Omniamid PA6 G G - Dry
Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, su..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
96.0
°C <br>@Thickness 0.125 mm
|
205
°F <br>@Thickness 0.00492 in
|
ASTM D648 |
|
Proto3000 PC-ABS Fused Deposition Modeling Polymer
Description: PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior strength and heat resis..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | Method A - Annealed; ASTM D-648 |
|
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | ISO 75-1/-2 |
|
Styrolution Luran® S KR 2867 C WU Colored ASA+PC
Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
|
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East)
CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | Method A - Annealed; ASTM D-648 |
|
Bhansali Engineering Abstron HCR-15 M ABS Heat Resistant
Chemical Resistant GradeInformation provided by Bhansali
|
|||