Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Boiling Point = 374 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Boiling Point 190 °C
374 °F
Dow Corning Z-6030 SILANE
Dow Corning® Z-6030 Silane is a bifunctional silane containing a methacrylate reactive organic group and a trimethoxysilyl inorganic group. The product is designated ?- methacryloxypropyltrimethoxy..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 223 Isocyanate
Description: Lupranate® 223 Isocyanate is a low viscosity derivative of both pure-MDI and polymeric-MDI. With a functionality of approximately 2.2, this isocyanate can be formulated into applicatio..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 224 Isocyanate
Description: Lupranate® 224 is a special medium viscosity polymeric MDI containing a high amount of 2,4'-diphenylmethane diisocyanate. The high 2,4'-MDI content will allow for better flow and lon..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 230 Isocyanate
Description: Lupranate® 230 Isocyanate is a low viscosity derivative of both pure-MDI and polymeric-MDI. With a functionality of approximately 2.2, this isocyanate can be formulated into applicatio..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 253 Isocyanate
Description: Lupranate® 253 Isocyanate is a solvent-free, modified pure diphenylmethane diisocyanate which is liquid at 30°C. It is designed to replace pure MDI in applications where it is desirab..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 265 Isocyanate
Description: Lupranate® 265 Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate 265 Isocyanate is used in the i..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 279 Isocyanate
Description: Lupranate® 279 Isocyanate is a 14% free-NCO prepolymer based on monomeric MDI chemistry. Lupranate 279 Isocyanate provides the lengthened open-time and high elongation desired in appli..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 3164T Isocyanate
Description: Lupranate® 3164T Isocyanate is a low viscosity polymeric MDI containing a high amount of diphenylmethane diisocyanate (monomeric MDI).Information provided by BASF
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 5050 Isocyanate
Description: Lupranate® 5050 Isocyanate is a prepolymer based on a modified, pure MDI. The intermediate free-NCO and slightly enhanced functionality of Lupranate 5050 isocyanate has benefited the f..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 5110 Isocyanate
Description: Lupranate® 5110 is a stable liquid polymeric MDI prepolymer. When used in molded flexible foams, Lupranate® 5110 Isocyanate demonstrates the ability to combine softness of foam with g..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® M20HB Isocyanate
Description: Lupranate® M20HB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20HB has faster reactivity than polymeric MDI currently used in the wood panel industry. Thi..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® MI Isocyanate
Description: Lupranate® MI Isocyanate is pure diphenylmethane diisocyanate containing a higher amount of 2,4´ isomer than Lupranate M Isocyanate or Lupranate MS Isocyanate. Lupranate MI Isocyanate..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® MS Isocyanate
Description: Lupranate® MS, a solid at room temperature, is essentially pure MDI and has a functionality of 2.0. Lupranate MS isocyanate is used in the isocyanate component for the preparation of e..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® R2500 Isocyanate
Description: Lupranate® R2500 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Careful control of the MDI distribution in Lupranate R2500 Isocyanate helps provide uniform re..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® TF2115 Isocyanate
Description: Lupranate® TF2115 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric-MDI) enriched with monomeric-MDI.Information provided by BASF
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 219 Isocyanate Modified MDI
Description: Lupranate® 219 Isocyanate is a liquid carbodiimide modified 4,4’-diphenylmethane diisocyanate. Lupranate 219 Isocyanate is a light-colored alternative to Lupranate MM103 Isocyanate. ..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 234 Isocyanate
Description: Lupranate® 234 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high 2,4’-MDI isomer content. Lupranate® 234 Isocyanate exhibits excellent low t..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 241 Isocyanate
Description: Lupranate® 241 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high2,4’-MDI isomer content. Lupranate® 241 Isocyanate exhibits excellent low t..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 274 Isocyanate
Description: Lupranate® 274 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Lupranate 274 Isocyanate is suitable for the production of rigid insulation foams by molding, sp..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 275 Isocyanate
Description: Lupranate® 275 Isocyanate is a 15.9% Free-NCO prepolymer based on diphenylmethane diisocyanate (MDI) chemistry. The formulation of Lupranate 275 Isocyanate provides the low viscosity a..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 281 Isocyanate
Description: Lupranate® 281 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric MDI) containing a very high amount of monomeric diphenylmethane diisocyanate (2,4'-MDI an..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 5060 Isocyanate
Description: Lupranate® 5060 Isocyanate is a low functional prepolymer based on monomeric MDI. Lupranate® 5060 isocyanate is suitable for use in a broad range of flexible, semi-flexible, and cast ..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 5070 Isocyanate
Description: Lupranate® 5070 Isocyanate is a low functional prepolymer based on pure MDI. Lupranate 5070 isocyanate is favored in solid elastomers and microcellular foams where the formulator desir..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 81 Isocyanate
Description: Lupranate® 81 Isocyanate is a carbodiimide modified pure MDI with a higher 2,4’-isomer content and a functionality of approximately 2.1. Lupranate 81 Isocyanate exhibits good low temp..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® LP27 Isocyanate
Description: Lupranate® LP27 Isocyanate is a special modified pure 4,4'-diphenylmethane diisocyanate that is a clear liquid at 27°C. Unlike pure 4,4'-MDI, Lupranate® LP27 Isocyanate has enhanced..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® M Isocyanate
Description: Lupranate® M Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate M Isocyanate is used in the isoc..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® M20FB Isocyanate
Description: Lupranate® M20FB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20FB has faster reactivity than polymeric MDI currently used in the wood panel industry. Thi..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® M20SB Isocyanate
Description: Lupranate® M20SB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20SB is a highly efficient, field-proven binder for cellulosic materials in products such as..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® 5080 Isocyanate
Description: Lupranate® 5080 Isocyanate is a 15.9% Free-NCO prepolymer based on diphenylmethane diisocyanate (MDI) chemistry. The formulation of Lupranate® 5080 Isocyanate provides the low viscosi..
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
BASF Lupranate® M10 Isocyanate
Description: Lupranate® M10 Isocyanate is a solvent-free polymeric MDI with a functionality of approximately 2.3. Lupranate M10 Isocyanate is a polymeric MDI which contains a relatively high level ..
Copyright © lookpolymers.com All Rights Reserved