| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay ALKAMULS® B Surfactant
Description: Ethoxylated castor oil Emulsifier for oil and waxes in water based formulations. Emulsifier for fats, oils, fatty acids, waxes and solvents. Used as dispersant for pigments and iron pow..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay ALKAMULS® OL 40 Surfactant
Identification: POLYOXYETHYLENE SORBITOL HEXAOLEATECAS: 057171 – 56 – 9Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Lat..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay ALKAMULS® OR 10 Surfactant
Identification: ETHOXYLATED CASTOR OILCAS: 61791 – 12 – 6Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay ALKAMULS® RC Surfactant
Identification: ETHOXYLATED CASTOR OILCAS: 61791 – 12 – 6Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay ANTAROX® V 27 Surfactant
Description: Linear Alcohol EO/PO.Identification: ETHO-PROPOXYLATED FATTY ALCOHOLCAS: 68603 - 25 – 8Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific,..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay GERONOL® PSI Surfactant
Description: Emulsifier for agrochemical formulations.Identification: BLENDED EMULSIFIERSSolubility: Soluble in water and most polar and aromatic solventsAvailable in: Asia Pacific, Europe, Latin Am..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay GEROPON® DOS/PG Surfactant
Identification: SODIUM DIOCTYLSULPHOSUCCINATE IN GLYCOL WATER SOLUTIONCAS: 577 – 11 – 7; 57 – 55 – 6; 7732 – 18 – 5Solubility: Dispersible in water and polar solvents. ..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay RHODAFAC® LO/529-E Surfactant
Identification: ETHOXYLATED ALKYLPHENOL PHOSPHATE, SODIUM SALT.CAS: 68954 – 84 – 7Solubility: Soluble in water and most aromatic solvents. Insoluble in polar solvents.Available in: Asia Pa..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | DIN/ISO 2562 |
|
Struktol STRUKSILON 8018 Silicone Stabilizer for PU-Microcellular Foam
STRUKSILON 8018 is used as a silicone stabilizer for the production of polyurethane microcellular foam. It is especially recommended for shoe sole formulations based on polyester and blends of polye..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | DIN/ISO 2562 |
|
Struktol STRUKSILON 8023 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8023 is a universal stabilizer for polyurethane rigid foams. It is especially recommended for the use in poor in place and roof sprayfoam applications.Applications: Information provided b..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay IGEPAL® OD 410 Surfactant
Description: Dispersant and emulsifier for cosmetic formulationsIdentification: ETHYLENE GLYCOL PHENYL ETHERC.T.F.A./INCI NAME: PHENOXYETHANOLCAS: 122 – 99 – 6Solubility: Insoluble in wate..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay RHODORSIL® EP 6703 Surfactant
Description: Antifoam for dry and liquid formulationsIdentification: ABSORBED POLYDIMETHYLSILOXANEAvailable in: Asia Pacific, Europe, Latin America and North America.Solubility: Dispersible in water..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay SIPOMER® WAM II Composition Based On Methacrylamidoethyl Ethylene Urea
Description: Specialty monomer for Wet Adhesion PromotionIdentification: COMPOSITION BASED ON METHACRYLAMIDOETHYL ETHYLENE UREACAS: 3089 – 19 – 8Solubility: Total in water Polymer Test (10..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay SOPROPHOR® BSU Surfactant
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED TRISTYRYLPHENOLCAS: 99734 – 09 – 5Solubility: Soluble in water and most polar and aromatic solvent..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay STANNINE® ETH Surfactant
Identification: BLEND OF CATIONIC SURFACTANTS IN WATERAvailable in: Asia Pacific, Europe, Latin America and North America Applications: Acid pickling inhibitor for HCl on ferrous metal. Effective ev..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | Closed cup |
|
Dow Corning FS 1265 Fluid, 300 CST
100% active, fluorosilicone polymer.Information provided by Dow Corning
|
|||
| Flash Point | 100 °C | 212 °F | closed cup |
|
Dow Corning SYL-OFF® 7791 RELEASE MODIFIER
Syl-Off® 7791 Release Modifier is a 100% active solids release modifier. A High efficiency release modifier suitable for use with Syl-Off® 7040 Coating.Information provided by Dow Corning
|
|||
| Flash Point | <= 100 °C | <= 212 °F | Closed cup |
|
Dow Corning SYL-OFF® PMCP7041 Modifier
Syl-Off® 7041 Release Modifier is a 100% active solids release modifier compatible with hexenyl functional polymers. Offers paricularly stable release and fast cure. Recommeded for use with Syl-Off..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | Closed cup |
|
Dow Corning SYL-OFF® PMCPEM 7974 Emulsion Coating
Syl-Off® EM 7974 is an emulsion based silicone release coating, excellent for bakery release performance and is specifically developed for application during the paper making process.Information pr..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | closed cup |
|
Dow Corning SYL-OFF® SL 9111 COATING
Syl-Off® SL 9111 Coating is a solvent-free, low temperature cure release coating for filmic pressure sensitive laminate/labelstock.Information provided by Dow Corning
|
|||
| Flash Point | >= 100 °C | >= 212 °F | Closed Cup |
|
Dow Corning XIAMETER® PMCPPMX-200 60,000CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 60,000CS. 100% active, 60,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
|
|||
| Flash Point | >= 100 °C | >= 212 °F | Closed cup |
|
Dow Corning 360 Medical Fluid, 100 CST.
Colorless and odorless polydimethysiloxane fluid for lubrication and siliconization of glass, metals, plastics and rubber in medical applications.Information provided by Dow Corning
|
|||
| Flash Point | 100 °C | 212 °F | ASTM-D3278 |
|
Abatron Abokote 8106-1 Water-Based Epoxy Coating for Floors
Abokote 8106-1 is a water-based epoxy coating that is part of the Abokote 8106-1 Flooring System which consists of this water-based epoxy coating, vinyl color chips, and Abokote 57-1 clear acrylic t..
|
|||
| Flash Point | 100 °C | 212 °F | ASTM-D3278 |
|
Abatron Water Epoxy Floor Coating System
The Water Epoxy Floor Coating System combines beauty, durability, slip resistance, ease of application, and water resistance. Its other features and benefits include low odor on installation, easy m..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay RHODAFAC® PA23 Surfactant
Description: Ethoxylated phosphate ester. Dispersing, wetting agent useful in suspension concentrates. Anionic emulsifier for industrial formulations. Used in a variety of applications from polyacry..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay RHODASURF® DA-630 E Surfactant
Description: Rhodapon® LS-92/RN is high purity, dust free anioinic surfactant in a needle form. Free flowing and easily dispersed in water. Excellent foaming and detergent properties.Identification..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay RHODOCLEAN® ASP Surfactant
Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Applications: Surfactant for metal working app..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay RHODOCLEAN® MSC Surfactant
Identification: ETHOXYL-PROPOXYL TERPENECAS: 174955 – 61 – 4Available in: Asia Pacific, Europe and Latin AmericaSolubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents..
|
|||
| Flash Point | >= 100 °C | >= 212 °F | |
|
Solvay SOPROPHOR® TS/16 Surfactant
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED TRISTYRYLPHENOLCAS: 104376 – 75 – 2Solubility: Soluble in water and most polar and aromatic solvents.Avail..
|
|||