| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flash Point | >= 170 °C | >= 338 °F | in closed cup |
|
Kazanorgsintez Polyethyleneglycol, Dust Controller
Production Method: Obtained by interaction of ethylene glycol and ethylene oxide. Application: Used as a reagent in production of potash fertilizers to reduce dust formation.Information Provided by ..
|
|||
| Flash Point | 170 °C | 338 °F | |
|
Solvay STANNINE® 5525 Surfactant
Description: Blend of substituted thiourea and surfactantsIdentification: ACID PICKLING INHIBITOR (SUBSTITUTED THIOUREA)CAS: 61791 – 00 – 2Solubility: Complete in acidsAvailable in: Asia P..
|
|||
| Flash Point | 170 °C | 338 °F | ASTM D93, DIN 51 755 |
|
Chesterton 390 Cutting Oil
Description: Chesterton® 390 Cutting Oil is a heavy duty, multi-purpose cutting fluid designed to provide maximum tool life and superior parts finish in severe applications. It is a highly reinforc..
|
|||
| Flash Point | 170 °C | 338 °F | |
|
Chesterton OPTICOOL™ 372 Lubrication
Description: OPTICOOL 372 is a proven, universal, water miscible metal working fluid. It is ideal where lubricity is important and operations severe. The 372 is suitable for a broad range of metal c..
|
|||
| Flash Point | 170 °C | 338 °F | PMCC; ASTM D92 |
|
ExxonMobil Exterex™ A34 Synthetic Fluid
Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol..
|
|||
| Flash Point | >= 170 °C | >= 338 °F | |
|
Unipetrol Light Oil Hydrogenate
Oil hydrogenates are a fraction boiling at above approximately 300°C, gained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of semi-soli..
|
|||