Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled  (discontinued **)
Hi-temp, waterborne silicone adhesive and sealant used to pot fiber optic strands into stainless steel ferrules. Typically used in applications to 716 °F (380 °C). Low viscosity, easy to use, offe..
Flash Point >= 100 °C
>= 212 °F
DIN/ISO 2562
Struktol STRUKSILON 8120 Silicone Stabilizer for PU Foam
STRUKSILON 8120 was developed as universal silicone stabilizer of high potency for the production of conventional as well as flame retardant flexible polyurethane slabstock foam based on polyether p..
Flash Point >= 100 °C
>= 212 °F
Solvay ALKAMULS® R 81 Surfactant
Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 9.Chemical Name: ETHOXYLATED CASTOR OILCAS: 61791 - 12 – 6Solubil..
Flash Point >= 100 °C
>= 212 °F
Solvay ANTAROX® PLG 254 Surfactant
Description: EO.PO block polymer. Multipurpose dispersing agent for suspension concentrate.Chemical Name: ETHYLENE/PROPYLENE OXIDE BLOCK POLYMERSolubility: Soluble in water and most polar solvents. ..
Flash Point >= 100 °C
>= 212 °F
Solvay GEROPON® SDS Surfactant
Description: Sodium dioctylsulfosuccinate. Low rate, high performance, wetting agent for dry formulations.Identification: SODIUM DIOCTYLSULPHOSUCCINATECAS: 577 – 11 – 7Solubility: Soluble..
Flash Point >= 100 °C
>= 212 °F
Solvay GEROPON® T/36 Surfactant
Identification: SODIUM POLYCARBOXYLATESolubility: Soluble in water. Insoluble in polar and aromatics solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Dispers..
Flash Point >= 100 °C
>= 212 °F
Solvay LUBRHOPHOS® LP 700 E Surfactant
Identification: POLYOXYETHYLENE PHENYL PHOSPHATE ESTER, ACID FORM.CAS: 39464 – 70 – 5Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, L..
Flash Point >= 100 °C
>= 212 °F
DIN/ISO 2562
Struktol STRUKSILON 8010 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8010 is a specialized stabilizer for polyurethane rigid foams. Due to its extremely good nucleating performance it is especially recommended for the production of foams with a very fine c..
Flash Point >= 100 °C
>= 212 °F
DIN/ISO 2562
Struktol STRUKSILON 8026 Silicone Stabilizer for PU Foam
STRUKSILON 8026 is used as a silicone stabilizer for the production of polyurethane shoe sole systems as well as other microcellular foams. It is especially recommended for shoe sole formulations ba..
Flash Point >= 100 °C
>= 212 °F
DIN/ISO 2562
Struktol STRUKSILON 8030 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8030 is a universal stabilizer for the production of polyurethane rigid foams. Due to its excellent flow properties and the very good insulation values that can be achieved STRUKSILON 803..
Flash Point >= 100 °C
>= 212 °F
DIN/ISO 2562
Struktol STRUKSILON 8101 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8101 is used as a silicone stabilizer for production of polyurethane rigid foam. It is especially recommended for the use in PU-1- or PU-2-component spray foam applications.Applications: ..
Flash Point >= 100 °C
>= 212 °F
Solvay SOPROPHOR® CY/8 Surfactant
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED TRISTYRYLPHENOLCAS: 99734 – 09 – 5Solubility: Soluble in water and most polar and aromatic solvent..
Flash Point >= 100 °C
>= 212 °F
Solvay SOPROPHOR® FL/60 Surfactant
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED POLYARYLPHENOL PHOSPHATE AMINE SALTSolubility: Soluble in water and most polar solvents. Insoluble in aromat..
Flash Point >= 100 °C
>= 212 °F
open cup
Dow Corning 772 WATER REPELLENT
Dow Corning® 777 Water Repellent is a water-dilutable solution of potassium methyl siliconate designed to impart water repellency to a wide variety of surfaces. Supplied at a concentration of 40 pe..
Flash Point >= 100 °C
>= 212 °F
closed cup
Dow Corning D94-20P A&B KIT
Two-part, 1:1 ratio, addition cure silicone elastomer for automated assembly of integrated compression sealsInformation provided by Dow Corning
Flash Point 100 °C
212 °F
closed cup
Dow Corning SYL-OFF® 7395 COATING
Syl-Off® 7395 Coating is a 100% active solids pre-catalysed, coating containing a low viscosity vinyl endblocked only functional silicone polymer. Provides a smooth, premium release performance, su..
Flash Point >= 100 °C
>= 212 °F
closed cup
Dow Corning SYL-OFF® 7673 COATING
Syl-Off® 7673 Coating is a 100% active solids pre-catalysed, coating containing a medium viscosity vinyl endblocked only functional silicone polymer. Provides a particularly smooth, premium release..
Flash Point 100 °C
212 °F
closed cup
Dow Corning SYL-OFF® 7780 RELEASE MODIFIER
Syl-off® 7780 Release Modifier is a 100% active solids, pre-catalysed, release modifier. High efficiency release modifier suitable for use with Syl-off® brand silicone release coatings.Information..
Flash Point >= 100 °C
>= 212 °F
closed cup
Dow Corning SYL-OFF® EM 7975 CATALYST EMULSION
Syl-Off® EM 7975 is an emulsion based silicone catalyst that provides excellent bakery release performance, and is specifically developed for application during the paper making process.Information..
Flash Point 100 °C
212 °F
Closed cup
Dow Corning SYL-OFF® PMCP7010 Coating
Syl-Off® 7010 Coating is a 100% active solids pre-catalysed, coating containing a low viscosity vinyl endblocked only functional silicone polymer. Provides a smooth, premium release performance and..
Flash Point >= 100 °C
>= 212 °F
Closed cup
Dow Corning SYL-OFF® PMCPEM 7974 Emulsion Coating
Syl-Off® EM 7974 is an emulsion based silicone release coating, excellent for bakery release performance and is specifically developed for application during the paper making process.Information pr..
Flash Point >= 100 °C
>= 212 °F
Closed cup
Dow Corning SYL-OFF® PMCPSL 9104 Coating
Syl-Off® SL 9104 Coating is a solvent-free silicone release coating for polyester substrates, providing excellent long-term anchorage to a wide range of both primed and unprimed polyester films.Inf..
Flash Point >= 100 °C
>= 212 °F
Closed Cup
Dow Corning XIAMETER® PMCPPMX-200 30,000CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 30,000CS. 100% active, 30,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Flash Point >= 100 °C
>= 212 °F
Closed cup
Dow Corning 360 Medical Fluid, 350 CST.
Colorless and odorless polydimethysiloxane fluid for lubrication and siliconization of glass, metals, plastics and rubber in medical applications.Information provided by Dow Corning
Flash Point >= 100 °C
>= 212 °F
B Component; ASTM D92
Aptek 6106-A/B Epoxy Encapsulant and/or Potting Compound
Optoelectronic grade encapsulant/potting compound – will not attack/cloud polysulphone casings. Lower Tg version, APTEK 6110-A/B, available for ceramic blob-top applications.Part A is hazy blue. Pa..
Flash Point >= 100 °C
>= 212 °F
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a..
Flash Point >= 100 °C
>= 212 °F
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Flash Point >= 100 °C
>= 212 °F
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Flash Point >= 100 °C
>= 212 °F
Solvay ABEX® EP 120 Surfactant
Description: Proprietary surfactant systemIdentification: ETHOXYLATED NONYLPHENOL SULPHATE AMMONIUM SALT WATER SOLUTIONCAS: 68649 – 55 – 8; 7732-18-5Solubility: Soluble in water. Insoluble in pola..
Flash Point >= 100 °C
>= 212 °F
Solvay RHODASURF® CET 5 Surfactant
Identification: ETHOXYLATED OLEYL CETYL ALCOHOLCAS: 68920 – 66 – 1Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America an..