| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flash Point | >= 250 °C | >= 482 °F | |
|
Precision Polymer Engineering H80B Epichlorohydrin
Peroxide Cured, Epichlorohydrin Rubber, 75-85 °IRHD. Terpolymer of epichlorohydrin, ethylene oxide and an unsaturated monomer. To ASTM D2000 line call-out: M3CH608, A25, B14, EO16, EO36, F17. AS..
|
|||
| Flash Point | >= 250 °C | >= 482 °F | |
|
Precision Polymer Engineering P70B Polyacrylate Rubber
Polyacrylic or Polyacrylate Rubber, 65-75 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi..
|
|||
| Flash Point | >= 250 °C | >= 482 °F | |
|
Precision Polymer Engineering P90B Polyacrylate Rubber
Polyacrylic or Polyacrylate Rubber, 85-95 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil 632 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil Gargoyle Arctic 226 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil SAE 40 Mobilgard 1 SHC
Mobilgard 1 SHC by ExxonMobil is a supreme performance, synthetic diesel engine oil specifically formulated to address the needs of high power, distillate fueled diesel engines. It provides lubricat..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil SAE 40 Mobilgard M30 Series
Mobilgard M30 Series (M330 and M430) by ExxonMobil are premium, extra high performance 30 TBN engine oils designed for use in the most severe residual-fueled, medium-speed diesel engines used in mar..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil Teresstic 77
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
|
|||
| Flash Point | 250 °C | 482 °F | |
|
ConocoPhillips SynXPA® 100 R&O Oil
Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acti..
|
|||
| Flash Point | 250 °C | 482 °F | |
|
ChevronTexaco 68 Way Lubricant
Texaco Way Lubricants deliver value through:Excellent separation from metalworking coolants — The SKC (SKC Gleittechnik) coolant separation test showed excellent separation from a wide variety of c..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ChevronTexaco Delo® 400 SAE 40
Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated ..
|
|||
| Flash Point | 250 °C | 482 °F | |
|
ChevronTexaco Geotex® Ashless SAE 15W-40
Texaco Geotex Ashless is a high quality, bright stock-free, ashless, dispersant-type gas engine oil. It is manufactured using selected paraffinic base oils and an additive package containing a disp..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ChevronTexaco ISO 100 Machine Oil AW
FeaturesChevron Machine Oils AW are premium quality lubricants.They provide excellent antiwear protection, oxidation and corrosion inhibition, and foam and aeration suppression.They are excellent mu..
|
|||
| Flash Point | 250 °C | 482 °F | |
|
ChevronTexaco Rando® HD 100
Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ChevronTexaco RPM® SAE 30 Heavy Duty Motor Oil
Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ChevronTexaco Rykon® ISO 15 Premium Oil
FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion ..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ChevronTexaco SYMBOL 9250 Marine Engine Oil, SAE 40
FeaturesChevron Marine Engine Oil Symbol 9250 is a high quality, high performance engine oil.It is manufactured using highly refined, high viscosity index paraffinic base oils to meet the critical d..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ChevronTexaco Syntholube® ISO 68 Compressor Oil
FeaturesChevron Syntholube Compressor Oils are synthetic diester-based, oxidation resistant, compressor oils.ApplicationsChevron Syntholube Compressor Oils are used for portable and stationary rotar..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil 150 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil 20 Exxon XD-3
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil 320 Mobil DTE PM Series
Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil SAE 40 Mobilgard 1 SHC
Mobilgard 1 SHC by ExxonMobil is a supreme performance, synthetic diesel engine oil specifically formulated to address the needs of high power, distillate fueled diesel engines. It provides lubricat..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil Teresstic 77
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D-92 |
|
ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150
Description: ANDEROL FGC 150 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated with special additive packages that provide good thermal and oxidative stability to keep val..
|
|||
| Flash Point | 250 °C | 482 °F | |
|
ConocoPhillips El Mar® 3000 Oil SAE Grade 30
Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ChevronTexaco Delo® 3000 Marine Engine Oil, SAE 40
FeaturesChevron Marine Engine Oil Delo 3000 Marine is a high quality engine oils developed for use in a wide variety of medium speed trunk piston engines burning residual fuels.It is manufactured us..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ChevronTexaco Vistac® ISO 68 Way Oil D
FeaturesChevron Way Oils Vistac D are high quality lubricants designed to meet the critical lubrication demands for the slides and ways of machine tools.Chevron Way Oils Vistac D is formulated with ..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil 632 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..
|
|||
| Flash Point | 250 °C | 482 °F | ASTM D92 |
|
ExxonMobil 150 Mobil DTE PM Series
Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona..
|
|||
| Flash Point | 250 °C | 482 °F | |
|
ChevronTexaco Havoline® SAE 30 Motor Oil
All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib..
|
|||