| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flash Point | 272 °C | 522 °F | ASTM D92 |
|
ExxonMobil 320 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
|
|||
| Flash Point | 272 °C | 522 °F | ASTM D92 |
|
ExxonMobil Extra Heavy Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..
|
|||
| Flash Point | 272 °C | 522 °F | ASTM D92 |
|
ExxonMobil 412 Mobilgard 12 Series
Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T..
|
|||
| Flash Point | 272 °C | 522 °F | ASTM D92 |
|
ExxonMobil 320 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
|
|||
| Flash Point | 272 °C | 522 °F | ASTM D92 |
|
ExxonMobil 412 Mobilgard 12 Series
Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T..
|
|||
| Flash Point | 272 °C | 522 °F | ASTM D92 |
|
ExxonMobil Extra Heavy Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..
|
|||